Abstract

Phenolic foams (PFs) are considered excellent insulation materials owing to their flame retardancy and low thermal conductivity. However, their mechanical properties often lag behind those of other polymeric insulation materials. To fully exploit their properties and broaden end-use applications, the mechanical properties of PFs must be enhanced. In this study, various modifications were introduced into the PF matrix with the aim of enhancing its properties. The toughening effects of four additives: urea (U), nano clay (NC), sodium silicate (SS), and lignin (Li) were studied and compared. Changes that occurred in the density, cell morphology, thermal conductivity, compressive strength, and thermal stability after the addition of these fillers were analyzed. Both compressive strength and thermal stability increased with the inclusion of all additives, and the SS-toughened foam shows the biggest improvement. Li and NC addition resulted in a 34% improvement in compressive strength, while SS and U addition displayed increases of 52 and 11%, respectively. SS-toughened PF shows greater improvements in all of the important properties compared with those of the other toughened foams. Several PFs were prepared by changing the SS concentration to optimize the formulation, which yielded improvements in properties. The effects of SS concentration on density, thermal conductivity, and compressive strength were studied. The formulation with 0.37% sodium silicate concentration (PF-SS1) shows a 15% improvement in mechanical properties.

摘要

酚醛泡沫(PFs)因其阻燃性和低导热率而被认为是优异的保温材料。然而,它们的机械性能往往落后于其他聚合物保温材料。为了充分发挥其性能并拓宽最终用途应用范围,必须提高PFs的机械性能。在本研究中,对PF基体进行了各种改性,以提高其性能。研究并比较了四种添加剂:尿素(U)、纳米粘土(NC)、硅酸钠(SS)和木质素(Li)的增韧效果。分析了添加这些填料后密度、泡孔形态、导热率、抗压强度和热稳定性的变化。所有添加剂的加入均使抗压强度和热稳定性提高,其中SS增韧泡沫的改善最为显著。添加Li和NC使抗压强度提高了34%,而添加SS和U分别提高了52%和11%。与其他增韧泡沫相比,SS增韧PF在所有重要性能方面都有更大的改善。通过改变SS浓度制备了几种PFs以优化配方,从而改善了性能。研究了SS浓度对密度、导热率和抗压强度的影响。硅酸钠浓度为0.37%的配方(PF-SS1)的机械性能提高了15%。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/33ac/10831839/95809ee5f9ac/ao3c07967_0001.jpg

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验