Kavoor Sowmya, Ranjini M A, Aziz Naval Abdul, Ashok H K, Nadig Roopa R
Department of Conservative Dentistry and Endodontics, Dayananda Sagar College of Dental Sciences, Bengaluru, Karnataka, India.
J Conserv Dent Endod. 2024 Mar;27(3):310-314. doi: 10.4103/JCDE.JCDE_310_23. Epub 2024 Mar 6.
Teeth bleaching, although considered safe and conservative, cause microscopic changes in the tooth structure. The aim of this study is to evaluate the bleaching efficacy of carbamide peroxide (CP) bleaching gel when modified with the incorporation of bioactive glass (BG) and hydroxyapatite (HA) and its effect on enamel microhardness.
Forty-five maxillary incisors were decoronated, artificially stained and mounted in acrylic. The samples were divided into three groups of 15 each and subjected to the following bleaching protocol for 8 h/day at 37°C for 2 weeks: Group 1 - 16% CP, Group 2 - CP modified with BG, and Group 3 - CP modified with hydroxyapatite (HA). Spectrophotometric color assessment using CIE Lab* system and Vickers microhardness were assessed before and after bleaching. Data were analyzed using Student's paired -test and one-way ANOVA followed by Tukey's analysis.
There was a significant change in color (Lab*) in all the three groups when compared to the baseline values. However, no significant difference in the total color change (ΔE) was observed between the three groups. Enamel microhardness reduced significantly in the CP group, whereas it increased in the BG and HA group after bleaching. Scanning electron microscopy images of BG and HA groups showed crystalline deposits suggesting mineral deposition.
Addition of biomaterials can be a beneficial alternative to bleaching with CP alone, considering the increase in microhardness without hindering the bleaching action.
牙齿漂白虽被认为安全且保守,但会引起牙齿结构的微观变化。本研究旨在评估加入生物活性玻璃(BG)和羟基磷灰石(HA)后过氧尿素(CP)漂白凝胶的漂白效果及其对牙釉质显微硬度的影响。
45颗上颌切牙被截冠、人工染色并固定在丙烯酸树脂中。样本分为三组,每组15颗,在37℃下按照以下漂白方案每天漂白8小时,持续2周:第1组 - 16% CP,第2组 - 用BG改性的CP,第3组 - 用羟基磷灰石(HA)改性的CP。在漂白前后使用CIE Lab*系统进行分光光度颜色评估和维氏显微硬度评估。数据采用学生配对检验和单因素方差分析,随后进行Tukey分析。
与基线值相比所有三组的颜色(Lab*)均有显著变化。然而,三组之间在总颜色变化(ΔE)上未观察到显著差异。CP组的牙釉质显微硬度显著降低,而BG组和HA组在漂白后显微硬度增加。BG组和HA组的扫描电子显微镜图像显示有晶体沉积,提示有矿物质沉积。
考虑到在不阻碍漂白作用的情况下显微硬度增加,添加生物材料可能是单独使用CP漂白的有益替代方法。