Abstract

Bisphenol A (BPA) is widely used around the world in the production of Polycarbonate (PC) plastics. Notably, the ubiquitous 5-gallon water bottles in the UAE are primarily made of PC plastic, making them a significant concern as bottled water is the region's main supply of drinking water. These bottles undergo temperature variations during storage and transportation, potentially leading to harmful BPA (Bisphenol A) leaching. This study analyzed 40 PC 5-gallon water bottles from two local brands A and B, with 20 bottles per brand, under two conditions: room temperature and outdoor sunlight exposure for a month. BPA levels were assessed at 0, 15, and 30 days, following ethical approval. Liquid-liquid extraction and ELISA assays were conducted, with comprehensive kit validation. The results revealed a significant increase in BPA concentration over time, particularly in bottles exposed to elevated temperatures (Day 30 outdoor-stored samples exhibited the highest concentration at 9.05 ± 2.30 μg/L). Brand B consistently exhibited higher BPA concentrations across different samples and environments. This study emphasizes the link between BPA content and storage time, highlighting the need for preventive measures to reduce BPA exposure. Individuals should be aware of potential health risks associated with prolonged storage in plastic containers and consider safer alternatives.

摘要

双酚A(BPA)在全球范围内广泛用于聚碳酸酯(PC)塑料的生产。值得注意的是,阿联酋随处可见的5加仑水瓶主要由PC塑料制成,由于瓶装水是该地区饮用水的主要供应来源,这使得它们成为一个重大问题。这些瓶子在储存和运输过程中会经历温度变化,可能导致有害的双酚A(BPA)渗出。本研究分析了来自当地两个品牌A和B的40个PC 5加仑水瓶,每个品牌20个,在两种条件下:室温以及在户外阳光下暴露一个月。在获得伦理批准后,在第0、15和30天评估双酚A水平。进行了液-液萃取和酶联免疫吸附测定,并对试剂盒进行了全面验证。结果显示,随着时间的推移,双酚A浓度显著增加,特别是在暴露于高温的瓶子中(第30天户外储存的样品浓度最高,为9.05±2.30μg/L)。在不同样品和环境中,品牌B的双酚A浓度始终较高。本研究强调了双酚A含量与储存时间之间的联系,突出了采取预防措施以减少双酚A暴露的必要性。个人应意识到长期储存在塑料容器中可能存在的健康风险,并考虑更安全的替代品。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/6f2c/11396560/7d4f42d3341e/nje-14-1302-g001.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验