García-Moreno Martha Esperanza, Salmerón-Valdés Elias Nahum, Morales-Valenzuela Adriana Alejandra, Velázquez-Enríquez Ulises, Toral-Rizo Víctor Hugo, Lara-Carrillo Edith
Center for Research and Advanced Studies in Dentistry, School of Dentistry, Autonomous University of Mexico State, Toluca, Estado de México, México.
Saudi Dent J. 2024 Nov;36(11):1490-1494. doi: 10.1016/j.sdentj.2024.09.010. Epub 2024 Sep 10.
The purpose of the study was to compare the fluoride release in two conventional glass ionomer cements (Ionobond, Ketac Molar) and two resin-modified glass ionomer cements (Vitrebond, Fuji II LC) adapted with halloysite nanotubes preloaded with sodium fluoride at different concentrations.
In total, 96 samples were prepared and distributed into four control groups and eight experimental groups (5 % and 10 %). Totals of 10 % and 5 % of the total weight of ionomer powder needed to prepare the samples were replaced with nanotubes, preloaded at 2,000 parts per million, respectively. The experimental groups were followed for 120 days at seven time intervals. All the samples were stored at 37 °C.
All the experimental groups showed significant differences compared with the control groups; likewise, differences were observed between the concentrations of 5% and 10%.
The experimental groups (conventional and resin-modified glass ionomer cements adapted with preloaded nanotubes) released a higher and more constant amount of fluoride compared to the control groups.
本研究的目的是比较两种传统玻璃离子水门汀(Ionobond、Ketac Molar)和两种树脂改性玻璃离子水门汀(Vitrebond、Fuji II LC)在与不同浓度预载氟化钠的埃洛石纳米管适配后的氟释放情况。
总共制备了96个样本,并分为四个对照组和八个实验组(5%和10%)。制备样本所需的离子体粉末总重量的10%和5%分别被百万分之2000预载的纳米管替代。实验组在七个时间间隔内跟踪观察120天。所有样本均储存在37℃。
所有实验组与对照组相比均显示出显著差异;同样,在5%和10%的浓度之间也观察到了差异。
与对照组相比,实验组(适配预载纳米管的传统和树脂改性玻璃离子水门汀)释放出更高且更恒定的氟含量。