Xia Rui, Lei Jie, Luo Maoxuan, Xiao Yao
Luzhou Key Laboratory of Oral & Maxillofacial Reconstruction and Regeneration, The Affiliated Stomatology Hospital, Southwest Medical University, Luzhou, Sichuan, China.
Department of Chengbei Outpatient, The Affiliated Stomatology Hospital, Southwest Medical University, Luzhou, Sichuan, China.
PLoS One. 2025 Aug 7;20(8):e0328937. doi: 10.1371/journal.pone.0328937. eCollection 2025.
There is a lack of research on the bonding ability of attachments to fluorosis enamel. This study evaluates Er: YAG laser-assisted acid etching as a potential optimization protocol.
Twenty healthy teeth and ninety fluorotic teeth (Thylstrup-Fejerskov Index = 4) were divided into a control group (healthy enamel + acid etching) and a fluorotic group (acid etching 30/60/90 seconds vs. Er: YAG laser + acid etching). The enamel surface was analyzed using scanning electron microscopy, and the shear bond strength (SBS) of each group (n = 10/group) was tested.
Attachments exhibited higher SBS than brackets (P < 0.01). Laser-acid etching enhanced SBS compared to acid etching alone (P < 0.01). Laser-treated surfaces exhibited predominantly mixed fracture and resin cohesion fractures, in contrast to adhesive interface fractures and mixed fractures in the acid-only groups.
Er: YAG laser (100mJ/30 Hz) with 60 seconds acid etching achieves excellent bonding for fluorotic enamel attachments, restoring adhesion to healthy enamel levels while preventing over-etching damage. This protocol shows clinical potential for bonding fluorotic enamel.
关于附着体与氟斑牙釉质粘结能力的研究较少。本研究评估铒激光辅助酸蚀作为一种潜在的优化方案。
将20颗健康牙齿和90颗氟斑牙(Thylstrup-Fejerskov指数=4)分为对照组(健康釉质+酸蚀)和氟斑牙组(酸蚀30/60/90秒与铒激光+酸蚀)。使用扫描电子显微镜分析釉质表面,并测试每组(n=10/组)的剪切粘结强度(SBS)。
附着体的SBS高于托槽(P<0.01)。与单独酸蚀相比,激光-酸蚀增强了SBS(P<0.01)。与仅酸蚀组的粘结界面断裂和混合断裂相比,激光处理的表面主要表现为混合断裂和树脂内聚断裂。
铒激光(100mJ/30Hz)联合60秒酸蚀可实现氟斑牙釉质附着体的优异粘结,将粘结力恢复到健康釉质水平,同时防止过度酸蚀损伤。该方案在粘结氟斑牙釉质方面具有临床应用潜力。