Biocompatibility of standard and silica-free silicone rubber membrane oxygenators.

作者信息

Fountain S W, Duffin J, Ward C A, Osada H, Martin B A, Cooper J D

出版信息

Am J Physiol. 1979 Feb;236(2):H371-5. doi: 10.1152/ajpheart.1979.236.2.H371.

Abstract

Spiral coil membrane oxygenators made from either standard silicone rubber or silica-free silicone rubber were compared using three priming techniques. Standard priming, carbon dioxide priming, and denucleation priming were employed with each type of device. Four-hour venovenous membrane oxygenator perfusions were carried out on awake sheep anticoagulated with heparin. Virtually no differences were observed in any parameters measured between standard silicone rubber and filler-free silicone rubber membranes. Significantly greater platelet losses occurred during the first hour of perfusion with standard priming and with carbon dioxide priming than with denucleation priming, using either type of membrane. These experiments demonstrate that denucleation priming reduces platelet losses during extracorporeal membrane oxygenator perfusion, but that the use of filler-free silicone rubber does not improve the biocompatibility of the membrane.

摘要

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验