一种用于制备脱钙硬组织三微米厚切片的快速塑料包埋技术。

A rapid plastic embedding technique for preparation of three-micron thick sections of decalcified hard tissue.

作者信息

Kimmel D, Jee W S

出版信息

Stain Technol. 1975 Mar;50(2):83-6. doi: 10.3109/10520297509117039.

Abstract

A 24 hour start-to-finish method is described for the preparation of three-micron-thick sections of decalcified hard tissues. Following acetone dehydration, the tissue to be embedded is infiltrated under vacuum with a series of graded clearing solutions which approach the content of the final methyl methacrylate mixture. After overnight in a 35 C oven, the plastic is polymerized by four hours heating at 42 C. Three-micron-thick sections are then easily prepared by using a Jung microtome for high resolution histologic or detailed autoradiographic procedures.

摘要

本文描述了一种用于制备脱钙硬组织三微米厚切片的24小时全程方法。在丙酮脱水后,将待包埋的组织在真空中用一系列分级透明剂进行浸润,这些透明剂的成分接近最终甲基丙烯酸甲酯混合物的成分。在35℃烤箱中放置过夜后,通过在42℃加热4小时使塑料聚合。然后使用荣格切片机轻松制备三微米厚的切片,用于高分辨率组织学或详细的放射自显影程序。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验