Okazaki M, Aoba T, Doi Y, Takahashi J, Moriwaki Y
J Dent Res. 1981 Apr;60(4):845-9. doi: 10.1177/00220345810600041501.
Fluoridated hydroxyapatites were synthesized at 80 degrees C (pH 7.4) to study their crystallinity and solubility in relation to fluoride content. The crystallinity of fluoridated hydroxyapatities increased initially, then decreased, and finally increased again with the degree of fluoridation, whereas the decrease in relative solubility of fluoridated hydroxyapatites at 25 degrees C (pH 4.0) was proportional to the logarithm of the fluoride content.
在80摄氏度(pH值7.4)的条件下合成了含氟羟基磷灰石,以研究其结晶度和溶解度与氟含量的关系。含氟羟基磷灰石的结晶度起初增加,随后降低,最终又随氟化程度的增加而增加,而在25摄氏度(pH值4.0)时,含氟羟基磷灰石相对溶解度的降低与氟含量的对数成正比。