Suppr超能文献

双固化树脂水门汀:体外磨损及剩余双键数量、填料体积和光固化的影响

Dual-cure resin cements: in vitro wear and effect of quantity of remaining double bonds, filler volume, and light curing.

作者信息

Peutzfeldt A

机构信息

Department of Dental Materials, School of Dentistry, Faculty of Health Sciences, University of Copenhagen, Denmark.

出版信息

Acta Odontol Scand. 1995 Feb;53(1):29-34. doi: 10.3109/00016359509005941.

Abstract

The present study measured in vitro occlusal wear, quantity of remaining double bonds, and volumetric filler content of eight dual-cure resin cements. Furthermore, the effect of light curing on wear and quantity of remaining double bonds was evaluated. The filler content varied between 31 vol% and 66 vol%. In vitro wear varied between 30 microns and 65 microns, and quantity of remaining double bonds between 19% and 38% when resin cements had been both chemically cured and light cured. When light curing had been omitted, wear varied between 36 microns and 74 microns, and quantity of remaining double bonds between 25% and 56%. One resin cement did not harden when not cured by light. Light curing improved the wear resistance of three resin cements by up to 44% and reduced the quantity of remaining double bonds of six cements by up to 36%. A three-dimensional regression analysis found wear to decrease with decreasing quantity of remaining double bonds and increasing volumetric filler content. A negative correlation was shown between compressive strength and wear.

摘要

本研究测量了8种双固化树脂水门汀的体外咬合磨损、剩余双键数量和体积填料含量。此外,还评估了光固化对磨损和剩余双键数量的影响。填料含量在31体积%至66体积%之间变化。当树脂水门汀经过化学固化和光固化后,体外磨损在30微米至65微米之间变化,剩余双键数量在19%至38%之间。当省略光固化时,磨损在36微米至74微米之间变化,剩余双键数量在25%至56%之间。有一种树脂水门汀在未进行光固化时未硬化。光固化使三种树脂水门汀的耐磨性提高了44%,并使六种水门汀的剩余双键数量减少了36%。三维回归分析发现,磨损随着剩余双键数量的减少和体积填料含量的增加而降低。抗压强度与磨损之间呈负相关。