Low film thickness is critical to the clinical success of cemented castings. This study investigated the effect of luting agent-metal physico-chemical surface interactions on film thicknesses of representative luting agents. Control group luting agents were placed between two glass plates, as described by American Dental Association specifications 8, 61, and 66, and test group luting agents were positioned between glass and metal plates. The materials selected were zinc phosphate cement, polycarboxylate cement, glass ionomer cement, glass ionomer-composite resin hybrid cement and a resinous cement, with a type III gold alloy, a noble metal ceramic alloy, and a base metal ceramic alloy. A two-way analysis of variance and follow-up tests were done. The effects of the type of metal surface, type of cement, and their statistical interaction significantly affected film thickness (p < 0.0001). The type of cement had a greater affect on film thickness than the type of metal. A glass ionomer cement produced lower overall film thicknesses than other cement types, and a noble metal ceramic alloy created lower overall film thicknesses than other types of metal. American Dental Association specifications for cement film thickness did not accurately reflect normal cement use.
低粘结剂膜厚度对粘结铸造修复体的临床成功至关重要。本研究调查了粘结剂与金属之间的物理化学表面相互作用对代表性粘结剂膜厚度的影响。按照美国牙科协会规范8、61和66所述,将对照组粘结剂置于两块玻璃板之间,而将试验组粘结剂置于玻璃与金属板之间。所选材料为磷酸锌水门汀、聚羧酸锌水门汀、玻璃离子水门汀、玻璃离子复合树脂混合水门汀和树脂水门汀,以及Ⅲ型金合金、贵金属烤瓷合金和贱金属烤瓷合金。进行了双向方差分析和后续检验。金属表面类型、水门汀类型及其统计交互作用对膜厚度有显著影响(p < 0.0001)。水门汀类型对膜厚度的影响大于金属类型。玻璃离子水门汀产生的总体膜厚度低于其他水门汀类型,贵金属烤瓷合金产生的总体膜厚度低于其他金属类型。美国牙科协会关于水门汀膜厚度的规范不能准确反映水门汀的正常使用情况。