Dootz E R, Koran A, Craig R G
Department of Biologic and Materials Sciences, School of Dentistry, University of Michigan, Ann Arbor.
J Prosthet Dent. 1994 Apr;71(4):379-83. doi: 10.1016/0022-3913(94)90098-1.
This study compares the tensile strength, elongation, Shore-A hardness, and tear resistance of three silicone maxillofacial materials before and after aging to provide comparative data for evaluation of new or experimental elastomers. The materials evaluated were MDX-4-4210, Factor II (A-2186), and Cosmesil. Tests were conducted 24 hours after specimen preparation and were repeated after aging for 900 hours in a Weather-Ometer device. Five samples were made for each material under all test conditions. After testing, mean values were calculated for all materials under all test conditions and were compared by two-way analysis of variance and Tukey intervals at p < or = 0.05.
本研究比较了三种硅橡胶颌面材料在老化前后的拉伸强度、伸长率、邵氏 A 硬度和抗撕裂性,以为评估新型或实验性弹性体提供对比数据。所评估的材料为 MDX - 4 - 4210、Factor II(A - 2186)和 Cosmesil。在标本制备后 24 小时进行测试,并在 Weather - Ometer 设备中老化 900 小时后重复测试。在所有测试条件下,每种材料制作五个样本。测试后,计算所有材料在所有测试条件下的平均值,并通过双向方差分析和 Tukey 区间在 p≤0.05 时进行比较。