Suppr超能文献

镍钛形状记忆合金的耐腐蚀性测试

Corrosion resistance tests on NiTi shape memory alloy.

作者信息

Rondelli G

机构信息

CNR-ITM, Milano, Italy.

出版信息

Biomaterials. 1996 Oct;17(20):2003-8. doi: 10.1016/0142-9612(95)00352-5.

Abstract

The corrosion performances of NiTi shape memory alloys (SMA) in human body simulating fluids were evaluated in comparison with other implant materials. As for the passivity current in potentiostatic conditions, taken as an index of ion release, the values are about three times higher for NiTi than for Ti6Al4V and austenitic stainless steels. Regarding the localized corrosion, while plain potentiodynamic scans indicated for NiTi alloy good resistance to pitting attack similar to Ti6Al4V, tests in which the passive film is abruptly damaged (i.e. potentiostatic scratch test and modified ASTM F746) pointed out that the characteristics of the passive film formed on NiTi alloy (whose strength can be related to the alloy's biocompatibility) are not as good as those on Ti6Al4V but are comparable or inferior to those on austenitic stainless steels.

摘要

将镍钛形状记忆合金(SMA)与其他植入材料相比较,评估了其在人体模拟液中的腐蚀性能。至于恒电位条件下的钝化电流(作为离子释放指标),镍钛合金的值约为Ti6Al4V和奥氏体不锈钢的三倍。关于局部腐蚀,虽然普通动电位扫描表明镍钛合金具有与Ti6Al4V相似的良好抗点蚀能力,但在被动膜突然受损的试验(即恒电位划痕试验和改进的ASTM F746)中指出,镍钛合金上形成的被动膜的特性(其强度可能与合金的生物相容性有关)不如Ti6Al4V上的被动膜,但与奥氏体不锈钢上的被动膜相当或更差。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验