Miller R A, Brady J M, Cutright D E
J Biomed Mater Res. 1977 Sep;11(5):711-9. doi: 10.1002/jbm.820110507.
This study determined the difference in rate of degradation between pure polymers of lactic acid (pla), glycolic acid (PGA), and various ratios of copolymers of these two substances. Fast-cured and slow-cured polyglycolide was compared with copolymers of glycolide/lactide intermixed in ratios of 75:25, 50:50, and 25:75, as well as pure polylactide. A total of 420 rats were implanted with carbon-14 and tritium-labeled polymers in bone and soft tissue. At intervals of 1, 2, 3, 5, 7, 9, and 11 months, groups of five animals with the implants in bone and five with the implants in the abdominal wall were sacrificed. The implant area as well as tissue from the liver, spleen, kidney, lung and some muscle tissue was analyzed for radioactivity along with the urine and feces collected throughout the experiment. Half-lives of the different polymers and copolymers were calculated from the radioactivity present in the implant area for each time interval. Half-life of the polymers and copolymers decreased from 5 months for 100% PGA to 1 week with 50:50 PGA:PLA copolymer and rapidly increased to 6.1 months for 100% PLA. Fast-cured PGA had a half-life in tissue of 0.85 months. No difference in rate of degradation was seen in soft tissue or bone. No significant radioactivity was detected in urine, feces, or tissue samples. From this study, it is concluded that control of degradation rate of the implant could best be attained by varying the composition of PLA and PGA between 75% and 100% PLA along with a corresponding 25% to 0% PGA. This would provide a half-life range of the implant of from 2 weeks to 6 months.
本研究确定了纯乳酸(聚乳酸,PLA)、乙醇酸(聚乙醇酸,PGA)聚合物以及这两种物质不同比例共聚物之间的降解速率差异。将快速固化和慢速固化的聚乙醇酸与乙醇酸/丙交酯比例为75:25、50:50和25:75的共聚物以及纯聚丙交酯进行了比较。总共420只大鼠在骨骼和软组织中植入了碳-14和氚标记的聚合物。在1、2、3、5、7、9和11个月的时间间隔,处死每组五只在骨骼中植入和五只在腹壁中植入的动物。分析植入区域以及肝脏、脾脏、肾脏、肺和一些肌肉组织中的放射性,同时分析整个实验过程中收集的尿液和粪便。根据每个时间间隔植入区域中存在的放射性计算不同聚合物和共聚物的半衰期。聚合物和共聚物的半衰期从100%PGA的5个月降至50:50 PGA:PLA共聚物的1周,并迅速增加到100%PLA的6.1个月。快速固化的PGA在组织中的半衰期为0.85个月。在软组织或骨骼中未观察到降解速率的差异。在尿液、粪便或组织样本中未检测到显著的放射性。从这项研究可以得出结论,通过在75%至100%的PLA之间改变PLA和PGA的组成以及相应的25%至0%的PGA,可以最好地控制植入物的降解速率。这将使植入物的半衰期范围为2周至6个月。