Davies J P, Harris W H
Orthopaedic Biomechanics Laboratory, Massachusetts General Hospital and Harvard Medical School, Boston 02114.
J Appl Biomater. 1992 Summer;3(2):81-5. doi: 10.1002/jab.770030203.
To aid in cement removal during revision arthroplasty, it has been proposed to add methylene blue to bone cement to provide contrast between the cement and bone. However, it is essential that the fatigue strength of the cement not be reduced by the addition of the methylene blue. The effect of adding 1 mL of an aqueous 1% solution of methylene blue to one pack of Simplex P prepared in the standard fashion (uncentrifuged) was studied. We also measured the fatigue properties of centrifuged Simplex P with three different methylene blue preparations. We studied adding 1 mL of an aqueous 1% solution of methylene blue, 0.5 g of methylene blue powder, and 0.1 mL of a 10% solution of methylene blue per pack of Simplex P bone cement. Adding 1 mL of a 1% methylene blue solution to 40 g of Simplex P without centrifuging the cement after mixing produced a cement with a mean fatigue life comparable to the uncentrifuged Simplex P without the methylene blue. However, the fatigue data scatter was higher for the uncentrifuged methylene blue preparation. The optimum methylene blue impregnated cement preparation was produced by adding 1 mL of a 1% methylene blue solution to 40 g of Simplex P powder, mixing with chilled monomer, and centrifuging for 60 s. Sterile 1 mL vials of 1% methylene blue solution are available in the operating room.(ABSTRACT TRUNCATED AT 250 WORDS)
为了在翻修关节成形术中辅助去除骨水泥,有人提议在骨水泥中添加亚甲蓝,以使骨水泥与骨骼之间形成对比。然而,至关重要的是,添加亚甲蓝不能降低骨水泥的疲劳强度。研究了向以标准方式(未离心)制备的一包Simplex P骨水泥中添加1 mL 1%亚甲蓝水溶液的效果。我们还测量了用三种不同亚甲蓝制剂离心后的Simplex P的疲劳性能。我们研究了每包Simplex P骨水泥添加1 mL 1%亚甲蓝水溶液、0.5 g亚甲蓝粉末和0.1 mL 10%亚甲蓝溶液的情况。向40 g Simplex P中添加1 mL 1%亚甲蓝溶液且混合后不离心骨水泥,所得到的骨水泥平均疲劳寿命与未添加亚甲蓝且未离心的Simplex P相当。然而,未离心的亚甲蓝制剂的疲劳数据离散度更高。最佳的亚甲蓝浸渍骨水泥制剂是通过向40 g Simplex P粉末中添加1 mL 1%亚甲蓝溶液,与冷却的单体混合,并离心60秒制备而成。手术室中有无菌的1 mL 1%亚甲蓝溶液小瓶。(摘要截短于250字)