Kawano Fumiaki, Ohguri Takafumi, Ichikawa Tetsuo, Mizuno Iwate, Hasegawa Akira
Department of Removable Prosthodontics, Tokushima University, School of Dentistry, 3-18-15 Kuramoto-cho, Tokushima 770-8504, Japan.
Int J Prosthodont. 2002 May-Jun;15(3):243-7.
Composite resin teeth are more widely used than porcelain or acrylic resin teeth in the fabrication of removable dentures because of their high fracture toughness and high abrasion resistance. The purpose of this study was to evaluate the shock absorbability of commercially available artificial posterior teeth by the free drop-ball test with an accelerometer and to evaluate the Vickers hardness at the surface.
The tested artificial teeth included seven composite resin teeth, one acrylic resin tooth, and one porcelain tooth. Specimens were tested 50 hours after immersion in distilled water at 37 degrees C. The impact value and Vickers hardness were measured. A one-way analysis of variance was used to analyzed the data (P = .05).
The composite resin teeth showed an intermediate impact value between that of the acrylic resin tooth and the porcelain tooth. Among the artificial teeth investigated, the porcelain tooth showed the highest impact value. A significant difference in the impact value was observed between the porcelain tooth and the composite resin and acrylic resin teeth. However, no significant difference was observed among the composite resin teeth tested. A significant correlation was found between the impact values and the Vickers hardness of the artificial teeth.
The present findings suggest that composite resin teeth and acrylic resin teeth have a higher shock absorbability than porcelain teeth.
由于复合树脂牙具有较高的断裂韧性和耐磨性,在可摘义齿制作中比瓷牙或丙烯酸树脂牙应用更为广泛。本研究的目的是通过使用加速度计的自由落球试验评估市售人工后牙的减震能力,并评估其表面的维氏硬度。
受试的人工牙包括七颗复合树脂牙、一颗丙烯酸树脂牙和一颗瓷牙。将试件在37℃蒸馏水中浸泡50小时后进行测试。测量冲击值和维氏硬度。采用单因素方差分析对数据进行分析(P = 0.05)。
复合树脂牙的冲击值介于丙烯酸树脂牙和瓷牙之间。在所研究的人工牙中,瓷牙的冲击值最高。瓷牙与复合树脂牙和丙烯酸树脂牙的冲击值存在显著差异。然而,在所测试的复合树脂牙之间未观察到显著差异。人工牙的冲击值与维氏硬度之间存在显著相关性。
目前的研究结果表明,复合树脂牙和丙烯酸树脂牙比瓷牙具有更高的减震能力。