不同增塑剂储存的红细胞中的生化和结构变化:己醇的作用。

Biochemical and structural changes in RBCs stored with different plasticizers: the role of hexanol.

作者信息

Draper C J, Greenwalt T J, Dumaswala U J

机构信息

Hoxworth Blood Center, University of Cincinnati Medical Center, Ohio 45267-0055, USA.

出版信息

Transfusion. 2002 Jul;42(7):830-5. doi: 10.1046/j.1537-2995.2002.00138.x.

Abstract

BACKGROUND

PVC containers are plasticized with di(2-ethyl)hexylphthalate (DEHP) or a related phthalate. The toxicity of DEHP has been questioned. It has been proposed to use butyryltrihexylcitrate (BTHC) as the plasticizer. The purpose of this study was to determine if hexanol, a component of BTHC, plays a role in the preservation of RBCs stored in BTHC-plasticized PVC bags.

STUDY DESIGN AND METHODS

WBC-reduced RBCs of ABO- and D-matched blood groups were prepared in 1-L polyolefin (PO) bags (PL732). Six 60-g aliquots were transferred to transfer packs made of PL146 (DEHP-plasticized) and PL2209 (BTHC-plasticized) and four PO (PL732) packs. To the PL146 and PL2209 packs, 30 mL of AS-1 was added. To three of the PO packs, 30 mL of AS-1 with sufficient DEHP, BTHC, or hexanol to achieve a final concentration of 3 mM was added, and to the final PO pack, 30 mL of AS-1 only was added (control). The units were stored for 6 weeks at 1 to 6 degrees C. RBC ATP, hemolysis, morphology, membrane lipids, deformability, and fluidity were measured.

RESULTS

ATP levels were not significantly different in any of the systems after 6 weeks. Compared to the PO bags, hemolysis was lowest in the PL146 containers and was also significantly lower (p < 0.006) in the PO bags with added DEHP, BTHC, or hexanol. The accumulation of vesicles was significantly less in the units stored in the PL146 and PL2209 than in the PO plastic with or without added plasticizers or hexanol (p < or = 0.004). There was no significant difference in the formation of vesicles in any of the PO units (p > 0.05). There was no demonstrable change in the membrane fluidity of the RBCs during storage in any of the systems. The decrease in deformability was the same, and the losses of cholesterol and phospholipid during storage were similar in all the studies.

CONCLUSIONS

The hexanol component of the BHTC plasticizer in a concentration of 144.6 microg per mL concentration suppresses hemolysis and vesiculation of RBCs during storage. The hexanol and DEHP that are slowly leached during storage have a greater effect in suppressing hemolysis and vesicle formation than when added extraneously to AS-1 in PO containers.

摘要

背景

聚氯乙烯(PVC)容器用邻苯二甲酸二(2 - 乙基)己酯(DEHP)或相关邻苯二甲酸盐增塑。DEHP的毒性受到质疑。有人提议使用柠檬酸丁酰三己酯(BTHC)作为增塑剂。本研究的目的是确定BTHC的成分己醇是否在保存在BTHC增塑的PVC袋中的红细胞保存中起作用。

研究设计与方法

在1升聚烯烃(PO)袋(PL732)中制备ABO血型和D抗原匹配的白细胞去除红细胞。将六个60克的等分试样转移到由PL146(DEHP增塑)和PL2209(BTHC增塑)制成的转移包以及四个PO(PL732)包中。向PL146和PL2209包中加入30毫升AS - 1。向三个PO包中加入30毫升AS - 1以及足量的DEHP、BTHC或己醇,使其最终浓度达到3 mM,向最后一个PO包中仅加入30毫升AS - 1(对照)。这些样本在1至6摄氏度下保存6周。测量红细胞的三磷酸腺苷(ATP)、溶血、形态、膜脂质、变形性和流动性。

结果

6周后,任何系统中的ATP水平均无显著差异。与PO袋相比,PL146容器中的溶血最低,并且在添加了DEHP、BTHC或己醇的PO袋中溶血也显著更低(p < 0.006)。储存在PL146和PL2209中的样本中囊泡的积累明显少于添加或未添加增塑剂或己醇的PO塑料中的样本(p ≤ 0.004)。任何PO样本中囊泡的形成均无显著差异(p > 0.05)。在任何系统中储存期间,红细胞的膜流动性均无明显变化。所有研究中变形性的降低相同,储存期间胆固醇和磷脂的损失相似。

结论

浓度为每毫升144.6微克的BHTC增塑剂中的己醇成分可抑制储存期间红细胞的溶血和囊泡形成。储存期间缓慢浸出的己醇和DEHP在抑制溶血和囊泡形成方面比在PO容器中向AS - 1中额外添加时具有更大的作用。