Pavarina A C, Vergani C E, Machado A L, Giampaolo E T, Teraoka M T
Department of Dental Materials and Prosthodontics, São Paulo State University (UNESP), Araraquara Dental School, Araraquara, SP, Brazil.
J Oral Rehabil. 2003 Jul;30(7):749-52. doi: 10.1046/j.1365-2842.2003.01145.x.
This investigation studied the effects of disinfectant solutions on the hardness of acrylic resin denture teeth. The occlusal surfaces of 64 resin denture teeth were ground flat with abrasives up to 400-grit silicon carbide paper. Measurements were made after polishing and after the specimens were stored in water at 37 degrees C for 48 h. The specimens were then divided into four groups and immersed in chemical disinfectants (4% chlorhexidine; 1% sodium hypochlorite and sodium perborate) for 10 min. The disinfection methods were performed twice to simulate clinical conditions and hardness measurements were made. Specimens tested as controls were immersed in water during the same disinfection time. Eight specimens were produced for each group. After desinfection procedures, testing of hardness was also performed after the samples were stored at 37 degrees C for 7, 30, 60, 90 and 120 days. Data were analysed using two-way analysis of variance (anova) and Tukey's test at 95% confidence level. According to the results, no significant differences were found between materials and immersion solutions (P > 0.05). However, a continuous decrease in hardness was noticed after ageing (P < 0.05). It was conclude that the surfaces of both acrylic resin denture teeth softened upon immersion in water regardless the disinfecting solution.
本研究调查了消毒溶液对丙烯酸树脂义齿牙齿硬度的影响。用粒度达400目的碳化硅砂纸将64颗树脂义齿牙齿的咬合面磨平。在抛光后以及将标本在37℃水中储存48小时后进行测量。然后将标本分为四组,浸入化学消毒剂(4%洗必泰;1%次氯酸钠和过硼酸钠)中10分钟。消毒方法重复进行两次以模拟临床情况,并进行硬度测量。作为对照测试的标本在相同消毒时间内浸入水中。每组制作8个标本。在消毒程序后,还在样本于37℃储存7、30、60、90和120天后进行硬度测试。使用双向方差分析(anova)和95%置信水平的Tukey检验对数据进行分析。根据结果,材料和浸泡溶液之间未发现显著差异(P>0.05)。然而,老化后硬度持续下降(P<0.05)。得出的结论是,无论消毒溶液如何,丙烯酸树脂义齿牙齿的表面在浸入水中后都会软化。