Joiner Andrew, Thakker Gopal, Cooper Yvonne
Unilever Oral Care, Quarry Road East, Bebington, Wirral, UK.
J Dent. 2004;32 Suppl 1:27-34. doi: 10.1016/j.jdent.2003.10.010.
The aims of this study were to evaluate the effects of a novel 6% hydrogen peroxide containing tooth whitener, Xtra White (XW), on enamel and dentine microhardness in vitro.
Polished human enamel and dentine specimens were prepared and baseline microhardness determined. In study 1, enamel specimens were exposed to 20 min cycles of either water, XW or Sprite Light for up to 28 cycles. In studies 2 and 3, enamel specimens were treated with 20 min cycles of either XW or water and exposed to whole saliva at all other times. In study 3, an additional exposure to a fluoride containing toothpaste was conducted. In total, 28 treatments were conducted in order to simulate a 2 weeks product use. In study 4, dentine specimens were treated as per study 3. Final microhardness measurements were taken and for studies 3 and 4 colour measurements were additionally taken.
XW and water gave no statistically significant (p>0.05) changes in enamel and dentine microhardness after 28 treatments. Sprite Light gave a significant (p<0.00002) reduction in enamel microhardness after one 20 min treatment. XW showed significant bleaching of enamel and dentine specimens as compared to the water control.
XW does not have any significant effect on enamel and dentine microhardness.
本研究旨在评估一种新型含6%过氧化氢的牙齿美白剂Xtra White(XW)对体外牙釉质和牙本质显微硬度的影响。
制备抛光后的人牙釉质和牙本质标本,并测定基线显微硬度。在研究1中,牙釉质标本分别暴露于水、XW或无糖雪碧中,每次20分钟,共进行28个循环。在研究2和3中,牙釉质标本分别用XW或水处理,每次20分钟,其余时间暴露于全唾液中。在研究3中,额外进行了含氟牙膏的处理。总共进行28次处理以模拟两周的产品使用情况。在研究4中,牙本质标本按照研究3的方法进行处理。进行最终的显微硬度测量,在研究3和4中还额外进行了颜色测量。
经过28次处理后,XW和水对牙釉质和牙本质显微硬度的影响无统计学意义(p>0.05)。无糖雪碧在一次20分钟处理后使牙釉质显微硬度显著降低(p<0.00002)。与水对照组相比,XW使牙釉质和牙本质标本出现显著漂白。
XW对牙釉质和牙本质显微硬度无显著影响。