生物活性硅灰石/聚(3-羟基丁酸酯-co-3-羟基戊酸酯)复合支架的制备与表征

Fabrication and characterization of bioactive wollastonite/PHBV composite scaffolds.

作者信息

Li Haiyan, Chang Jiang

机构信息

Biomaterials and Tissue Engineering Research Center, Shanghai Institute of Ceramics, 1295 Dingxi Road, Shanghai 200050, China.

出版信息

Biomaterials. 2004 Nov;25(24):5473-80. doi: 10.1016/j.biomaterials.2003.12.052.

Abstract

Composite scaffolds of polyhydroxybutyrate-polyhydroxyvalerate (PHBV) with bioactive wollastonite were fabricated by a compression moulding, thermal processing, and salt particulate leaching method. Structure and mechanical properties of the scaffolds were determined. The bioactivity of the composites was evaluated by soaking in a simulated body fluid (SBF), and the formation of the hydroxyapatite (HAp) layer was determined by Scanning Electron Microscope (SEM) and Energy-Dispersive Spectrometer (EDS). The results showed that the wollastonite/PHBV composites were bioactive as it induced the formation of HAp on the surface of the composite scaffolds after soaking in SBF for 14 days. In addition, the measurements of the water contact angles suggested that incorporation of wollastonite into PHBV could improve the hydrophilicity of the composites and the enhancement was dependent on the wollastonite content. Furthermore, the pH and ion concentration changes of SBF solutions with composite scaffolds showed that the composites released Ca and Si ions, which could neutralize the acidic by-products of the PHBV and stabilize the pH of the SBF solutions between 7.2 and 7.8 within a 3-week soaking period. All of these results suggest that the incorporation of wollastonite was a useful approach to obtain composite scaffolds with improved properties.

摘要

采用模压、热加工和盐颗粒沥滤法制备了具有生物活性硅灰石的聚羟基丁酸酯-聚羟基戊酸酯(PHBV)复合支架。测定了支架的结构和力学性能。通过浸泡在模拟体液(SBF)中评估复合材料的生物活性,并通过扫描电子显微镜(SEM)和能谱仪(EDS)测定羟基磷灰石(HAp)层的形成。结果表明,硅灰石/PHBV复合材料具有生物活性,在SBF中浸泡14天后,其在复合支架表面诱导形成了HAp。此外,水接触角的测量表明,将硅灰石掺入PHBV中可以提高复合材料的亲水性,且增强程度取决于硅灰石含量。此外,含有复合支架的SBF溶液的pH值和离子浓度变化表明,复合材料释放出Ca和Si离子,这可以中和PHBV的酸性副产物,并在3周的浸泡期内将SBF溶液的pH值稳定在7.2至7.8之间。所有这些结果表明,掺入硅灰石是获得性能改善的复合支架的一种有效方法。