Suppr超能文献

近端直接复合树脂修复体和椅旁CAD/CAM嵌体:使用和不使用选择性釉质预处理的两步自酸蚀粘结剂的边缘适应性

Proximal direct composite restorations and chairside CAD/CAM inlays: marginal adaptation of a two-step self-etch adhesive with and without selective enamel conditioning.

作者信息

Bortolotto T, Onisor I, Krejci I

机构信息

Division of Cariology and Endodontology, School of Dental Medicine, University of Geneva, Geneva, Switzerland.

出版信息

Clin Oral Investig. 2007 Mar;11(1):35-43. doi: 10.1007/s00784-006-0076-x. Epub 2006 Oct 10.

Abstract

The aim of this study was to evaluate the marginal adaptation of CEREC ceramic inlays, CEREC composite inlays and direct composite restorations in unbeveled proximal slot cavities under artificial aging conditions. Two groups of each restoration type were prepared (n = 6), one group with a self-etch adhesive, the other group with H(3)PO(4) enamel etching before the self-etch adhesive application. Replicas were generated before and after long-term thermo-mechanical loading under dentinal fluid simulation and margins were evaluated at x200 magnification in the scanning electron miscroscope (SEM). Statistically, significant differences were found before and after loading with respect to the percentages of "continuous margins", the direct composite filling with H(3)PO(4) enamel etching giving the lowest percentages of "continuous margins" after loading (p < 0.05). The highest percentage of "continuous margin" was attained by composite inlays without H(3)PO(4) enamel etching. However, these results were not significantly different from ceramic inlays after stressing. Polymerization shrinkage is still one critical property of composite restorative materials. The marginal adaptation of indirect adhesive proximal slot restorations without enamel bevels both fabricated out of composite and ceramic is better than that of directly placed composite restorations.

摘要

本研究的目的是评估在人工老化条件下,CEREC陶瓷嵌体、CEREC复合树脂嵌体和直接复合树脂修复体在未做斜面的邻面窝洞中的边缘适合性。每种修复类型制备两组(n = 6),一组使用自酸蚀粘结剂,另一组在应用自酸蚀粘结剂之前先用H₃PO₄酸蚀牙釉质。在模拟牙本质液的长期热机械加载前后制作复制件,并在扫描电子显微镜(SEM)下以200倍放大率评估边缘。统计学上,加载前后在“连续边缘”百分比方面发现了显著差异,加载后用H₃PO₄酸蚀牙釉质的直接复合树脂充填体的“连续边缘”百分比最低(p < 0.05)。未用H₃PO₄酸蚀牙釉质的复合树脂嵌体获得的“连续边缘”百分比最高。然而,在受力后这些结果与陶瓷嵌体没有显著差异。聚合收缩仍然是复合树脂修复材料的一个关键特性。由复合树脂和陶瓷制成的无牙釉质斜面的间接粘结邻面窝洞修复体的边缘适合性优于直接放置的复合树脂修复体。