Soares Carlos José, Santana Fernanda R, Silva Natércia R, Preira Janaína C, Pereira Cristina A
Department of Operative Dentistry and Dental Materials, Dental School, Federal University of Uberlândia, Uberlândia, Minas Gerais, Brazil.
J Endod. 2007 May;33(5):603-6. doi: 10.1016/j.joen.2007.01.016. Epub 2007 Mar 26.
This study evaluated the effect of endodontic treatment and storage time on the flexural and ultimate tensile strength of root dentin. Eighty bovine teeth were divided into endodontically treated (ET) and endodontically untreated (NT) teeth. The ET canals were instrumented and irrigated with sodium hypochlorite 1.0%. Roots were filled with gutta-percha and zinc-oxide/eugenol cement by the lateral condensation technique. Tests were performed as follows: t1, immediately; t2, 7 days; t3, 15 days; and t4, 30 days after extraction for NT groups or after extraction and endodontic treatment for ET groups (n= 0). Roots were axially cut into two halves, one half was used to obtain bars for performing the four-bending flexural test and the other half to obtain slices that were trimmed resulting in hourglass-shaped specimens for microtensile testing. Samples were submitted to the tests, and the data were statistically analyzed. Results indicated that endodontic treatment potentiated by time elapsed after endodontic treatment can affect the physical properties of dentin.
本研究评估了根管治疗和储存时间对牙根牙本质弯曲强度和极限拉伸强度的影响。80颗牛牙被分为根管治疗组(ET)和未进行根管治疗组(NT)。对ET组根管进行预备,并用1.0%的次氯酸钠冲洗。采用侧向加压技术用牙胶和氧化锌/丁香酚水门汀充填根管。测试按以下方式进行:NT组在拔牙后立即测试(t1)、拔牙后7天(t2)、拔牙后15天(t3)和拔牙后30天(t4);ET组在拔牙并完成根管治疗后相应时间测试(n = 0)。将牙根沿轴向切成两半,一半用于制备进行四点弯曲试验的试条,另一半用于制备切片,修整后得到沙漏形微拉伸试验样本。对样本进行测试,并对数据进行统计学分析。结果表明,根管治疗后经过的时间会增强根管治疗对牙本质物理性能的影响。