高交联聚乙烯与36毫米和28毫米股骨头磨损的放射性立体测量分析比较

Radiostereometric analysis comparison of wear of highly cross-linked polyethylene against 36- vs 28-mm femoral heads.

作者信息

Bragdon Charles R, Greene Meridith E, Freiberg Andrew A, Harris William H, Malchau Henrik

机构信息

Orthopaedic Biomechanics and Biomaterials Laboratory, Massachusetts General Hospital, Harvard Medical School, Boston, Massachusetts 02114, USA.

出版信息

J Arthroplasty. 2007 Sep;22(6 Suppl 2):125-9. doi: 10.1016/j.arth.2007.03.009. Epub 2007 Jul 26.

Abstract

This study used radiostereometric analysis (RSA) to compare the femoral head penetration of 28- vs 36-mm-diameter femoral heads into highly cross-linked polyethylene in 2 groups of total hip arthroplasty patients. Thirty patients were enrolled in this RSA study using highly cross-linked polyethylene (Longevity, Zimmer Inc, Warsaw, Idaho) against either 28- or 36-mm-diameter cobalt chrome femoral heads. At 3-year follow-up, there was no significant difference in the total average femoral head penetration, including both creep and wear, using 3 methods of RSA measurement between the 2 groups. Importantly, after bedding-in, there was no further significant increase in the amount of femoral head penetration (ie, wear) with either head size between years 1 and 3. There were no radiographic signs of lysis or radiolucencies at a minimum 3-year follow-up.

摘要

本研究采用放射立体测量分析(RSA),比较了两组全髋关节置换术患者中,直径28毫米与36毫米的股骨头在高交联聚乙烯中的股骨头穿透情况。30名患者参与了这项使用高交联聚乙烯(Longevity,Zimmer公司,爱达荷州华沙)与直径28毫米或36毫米钴铬合金股骨头的RSA研究。在3年随访时,两组之间使用3种RSA测量方法得出的总平均股骨头穿透情况(包括蠕变和磨损)无显著差异。重要的是,在磨合后,1至3年间,两种股骨头尺寸下的股骨头穿透量(即磨损)均未进一步显著增加。在至少3年的随访中,没有出现溶解或透亮线的影像学迹象。