Suppr超能文献

新型镁蔷薇辉石陶瓷的制备及其体外生物活性

Preparation and in vitro bioactivity of novel merwinite ceramic.

作者信息

Ou Jun, Kang Yunqing, Huang Zhongbing, Chen Xianchun, Wu Jiang, Xiao Rongchi, Yin Guangfu

机构信息

School of Materials Science and Engineering, Sichuan University, Chengdu, 610064, People's Republic of China.

出版信息

Biomed Mater. 2008 Mar;3(1):015015. doi: 10.1088/1748-6041/3/1/015015. Epub 2008 Mar 3.

Abstract

The ceramic of merwinite (Ca3MgSi2O8) was prepared by sintering sol-gel-derived merwinite powder compacts. The mechanical properties and the coefficient of thermal expansion (CTE) of the merwinite ceramic were determined. In vitro bioactivity of the merwinite ceramics was evaluated. Our results showed that the sintered body was single-phase merwinite ceramic, and that its bending strength, fracture toughness and Young's modulus were approximately 151 MPa, 1.72 MPa m(1/2) and 31 GPa, respectively. The CTE of the ceramic was 9.87 x 10(-6) degrees C(-1) and close to that for the Ti-6Al-4V alloy (9.80 x 10(-6) degrees C(-1)). Immersion of the sintered body in simulated body fluid induced surface precipitation of Ca-P rich layers. Cell culture experiment results confirmed that soluble ionic products from merwinite dissolution significantly stimulated osteoblast proliferation, and osteoblasts adhered and spread well on merwinite ceramic surfaces.

摘要

通过烧结溶胶 - 凝胶法制备的钙镁橄榄石(Ca3MgSi2O8)粉末压块来制备钙镁橄榄石陶瓷。测定了钙镁橄榄石陶瓷的力学性能和热膨胀系数(CTE)。评估了钙镁橄榄石陶瓷的体外生物活性。我们的结果表明,烧结体为单相钙镁橄榄石陶瓷,其弯曲强度、断裂韧性和杨氏模量分别约为151MPa、1.72MPa·m(1/2)和31GPa。该陶瓷的热膨胀系数为9.87×10(-6)℃(-1),与Ti - 6Al - 4V合金的热膨胀系数(9.80×10(-6)℃(-1))相近。将烧结体浸泡在模拟体液中会诱导富含Ca - P层的表面沉淀。细胞培养实验结果证实,钙镁橄榄石溶解产生的可溶性离子产物显著刺激成骨细胞增殖,并且成骨细胞在钙镁橄榄石陶瓷表面能够良好地附着和铺展。