Department of Conservative Dentistry, Hacettepe University, School of Dentistry, Ankara, Turkey.
Lasers Med Sci. 2010 Jul;25(4):511-6. doi: 10.1007/s10103-009-0682-3. Epub 2009 May 28.
This in vitro study evaluated the shear bond strength (SBS) of two self-etch adhesives to coronal and root dentin treated with erbium:yttrium-aluminum-garnet (Er:YAG) or neodymium:yttrium-aluminum-garnet (Nd:YAG) lasers for dentin hypersensitivity. The coronal and root dentin surfaces of 60 extracted human cuspids were divided into three groups (n = 20): (1) control (without treatment); (2) treated with Er:YAG; (3) treated with Nd:YAG laser and a one-step (S3) or two-step self-etch adhesive (SE). A nano-composite was applied and SBS tests were performed. The mean SBS values were calculated, failure modes were determined, and data were subjected to statistical analysis (P = 0.05). Control/SE exhibited higher values than did control/S3 and Nd:YAG/S3 on coronal dentin (P < 0.05). No significant differences were observed between the SE and S3 groups in root dentin (P > 0.05). Comparisons of two dentin substrates did not show any difference except control/SE (P < 0.05). The failure modes were mainly adhesive. The SBSs of self-etch adhesives to Er:YAG or Nd:YAG laser-treated surfaces were comparable with control for both coronal and root dentin.
钇铝石榴石(Er:YAG)或钕:钇铝石榴石(Nd:YAG)激光处理后的牙冠和牙根牙本质的剪切结合强度(SBS)。60 颗人尖牙的牙冠和牙根牙本质表面被分为三组(n = 20):(1)对照组(不处理);(2)Er:YAG 处理组;(3)Nd:YAG 激光处理组和一步(S3)或两步自酸蚀黏结剂(SE)处理组。应用纳米复合材料并进行 SBS 测试。计算平均 SBS 值,确定失效模式,并对数据进行统计分析(P = 0.05)。在牙冠牙本质上,与 S3 组相比,对照组/SE 组的 SBS 值高于对照组/S3 组和 Nd:YAG/S3 组(P < 0.05)。在牙根牙本质中,SE 组和 S3 组之间未观察到显著差异(P > 0.05)。除对照组/SE 组外(P < 0.05),两种牙本质基底之间的比较未显示出任何差异。失效模式主要为黏附性。对于 Er:YAG 或 Nd:YAG 激光处理后的牙本质,自酸蚀黏结剂的 SBS 与对照组相比,在牙冠和牙根牙本质中均具有可比性。