OBJECTIVES

This retrospective study evaluated the clinical performance and long-term survival of glass-ceramic lithium disilicate all-ceramic restorations in anterior and posterior areas over a 10-year period.

METHOD AND MATERIALS

Following a consistent protocol over 10 years, 261 lithium disilicate crowns (IPS Empress 2, Ivoclar Vivadent), including 101 anterior (38.7%) and 160 posterior (61.3%), were cemented using an adhesive technique and observed by the clinician who prepared and luted them. The data were analyzed using the Kaplan-Meier test. The clinical evaluation adopted the California Dental Association (CDA) modified criteria after recalling all patients between January and May 2008.

RESULTS

Six crowns failed and were replaced, 4 due to chipping and 2 due to core fracture. The overall survival rate was 95.5%.

CONCLUSION

In this retrospective evaluation, lithium disilicate ceramic restorations had a low clinical failure rate after up to 120 months.

摘要

目的

本回顾性研究评估了锂 disilicate 玻璃陶瓷全瓷修复体在前牙和后牙区域 10 年期间的临床性能和长期存活率。

方法和材料

在 10 年期间遵循一致的方案,使用粘结技术粘结了 261 个锂 disilicate 全冠(IPS Empress 2,义获嘉伟瓦登特),包括 101 个前牙全冠(38.7%)和 160 个后牙全冠(61.3%),并由制备和粘结它们的临床医生进行观察。使用 Kaplan-Meier 检验分析数据。在 2008 年 1 月至 5 月召回所有患者后,临床评估采用加利福尼亚牙科协会(CDA)修改后的标准。

结果

6 个全冠失败并被更换,4 个由于崩瓷,2 个由于核折裂。总体存活率为 95.5%。

结论

在本回顾性评估中,锂 disilicate 陶瓷修复体在长达 120 个月后临床失败率较低。