The main goal of the current study was to evaluate the surface roughness of tooth-colored restorative materials after different finishing/polishing protocols, including a liquid polisher (BisCover, BISCO, Schaumburg, IL, USA). The restorative materials tested included two nanofilled resin composites (Filtek Supreme, 3M Dental Products, St Paul, MN, USA and Grandio, Voco, Cuxhaven, Germany), one resin-modified glass ionomer cement (Vitremer, 3M Dental Products) and one conventional glass ionomer cement (Meron Molar ART, Voco). The finishing/polishing methods were divided into five groups: G1 (compression with Mylar matrix), G2 (finishing with diamond burs), G3 (Sof-Lex, 3M Dental Products), G4 (BisCover, BISCO, after diamond burs) and G5 (BisCover after Sof-Lex). Five cylindrical specimens of each material were prepared for each group according to the manufacturer's instructions. The finishing/polishing methods were performed by a single operator in one direction to avoid variations at low speed (15,000 RPM). The surface roughness was evaluated using a 3-D scanning instrument with two parameters considered (Ra and Rz). The data was analyzed using one-way ANOVA followed by a multiple comparison Tukey's test. The results showed that BisCover (BISCO) was capable of reducing surface roughness and provided polished surfaces for all materials, enhancing smoothness over already polished surfaces (Sof-Lex, 3M Dental Products) and achieving polishing after finishing with diamond burs.

摘要

本研究的主要目的是评估不同的修整/抛光方案(包括液体抛光机[BisCover,BISCO,Schaumburg,IL,美国])对牙色修复材料表面粗糙度的影响。测试的修复材料包括两种纳米复合树脂复合材料(Filtek Supreme,3M Dental Products,St Paul,MN,美国和Grandio,Voco,Cuxhaven,德国),一种树脂改性玻璃离子水门汀(Vitremer,3M Dental Products)和一种传统的玻璃离子水门汀(Meron Molar ART,Voco)。修整/抛光方法分为五组:G1(用聚酯薄膜基质压缩),G2(用金刚砂车针修整),G3( Sof-Lex,3M Dental Products),G4(先用金刚砂车针,再用 BisCover,BISCO)和 G5(先用 Sof-Lex,再用 BisCover,BISCO)。根据制造商的说明,每组每种材料制备五个圆柱形试件。修整/抛光方法由一名操作人员以一个方向进行,以避免低速(15000 RPM)时的差异。使用三维扫描仪器评估表面粗糙度,考虑两个参数(Ra 和 Rz)。使用单向方差分析(ANOVA)和多重比较 Tukey 检验对数据进行分析。结果表明,BisCover(BISCO)能够降低所有材料的表面粗糙度,并提供抛光表面,使表面光滑度超过已抛光表面(Sof-Lex,3M Dental Products),并在金刚砂车针修整后进行抛光。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验