亲水性聚酯微球:分子量和共聚物组成对 BSA 释放的影响。

Hydrophilic polyester microspheres: effect of molecular weight and copolymer composition on release of BSA.

机构信息

Department of Pharmaceutics, Utrecht Institute for Pharmaceutical Sciences (UIPS), Utrecht University, P.O. Box 80082, Sorbonnelaan 16, 3508 TB, Utrecht, The Netherlands.

出版信息

Pharm Res. 2010 Sep;27(9):2008-17. doi: 10.1007/s11095-010-0205-8. Epub 2010 Jul 3.

Abstract

PURPOSE

To study the release of a model protein, bovine serum albumin (BSA), from microspheres of an hydroxylated aliphatic polyester, poly(lactic-co-hydroxymethyl glycolic acid) (PLHMGA).

METHODS

BSA-loaded microspheres were prepared by a double emulsion solvent evaporation method. The effect of copolymer composition and the molecular weight of the copolymer on in vitro release and degradation were studied. The integrity of the released BSA was studied by fluorescence spectroscopy and size exclusion chromatography (SEC).

RESULTS

Microspheres prepared from PLHMGA with 50% hydroxymethyl glycolic acid (HMG) showed a burst release followed by a sustained release in 5-10 days. PLHMGA microspheres prepared from a copolymer with 35% and 25% HMG showed a sustained release of BSA up to 80% for 30 and 60 days, respectively. The release of BSA was hardly affected by the molecular weight of the polymer. Fluorescence spectroscopy and SEC showed that the released BSA preserved its structural integrity. Microspheres were fully degradable, and the degradation time increased from approximately 20 days to 60 days when the HMG content decreased from 50% to 25%.

CONCLUSIONS

Taking the degradation and release data together, it can be concluded that the release of BSA from PLHMGA microspheres is governed by degradation of the microspheres.

摘要

目的

研究模型蛋白牛血清白蛋白(BSA)从羟化脂肪族聚酯聚(乳酸-co-羟甲基聚乙二醇酸)(PLHMGA)微球中的释放情况。

方法

通过双乳液溶剂蒸发法制备载有 BSA 的微球。研究了共聚物组成和共聚物分子量对体外释放和降解的影响。通过荧光光谱法和尺寸排阻色谱法(SEC)研究了释放的 BSA 的完整性。

结果

含有 50%羟甲基聚乙二醇酸(HMG)的 PLHMGA 微球表现出突释,随后在 5-10 天内持续释放。由 35%和 25%HMG 的共聚物制备的 PLHMGA 微球分别持续释放 BSA 长达 30 和 60 天,达到 80%。BSA 的释放几乎不受聚合物分子量的影响。荧光光谱法和 SEC 表明释放的 BSA 保持其结构完整性。微球完全可降解,当 HMG 含量从 50%降低到 25%时,降解时间从大约 20 天增加到 60 天。

结论

综合降解和释放数据,可以得出结论,BSA 从 PLHMGA 微球中的释放受微球降解的控制。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/bb45/2916118/03f876723a23/11095_2010_205_Fig1_HTML.jpg

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验