Department of Crown and Bridge, School of Life Dentistry at Tokyo, The Nippon Dental University, Tokyo, Japan.
Int J Oral Sci. 2010 Mar;2(1):28-34. doi: 10.4248/IJOS10002.
To evaluate the interactive effects of different self-adhesive resin cements and tribochemical treatment on bond strength to zirconia.
The following self-adhesive resin cements for bonding two zirconia blocks were evaluated: Maxcem (MA), Smartcem (SM), Rely X Unicem Aplicap (UN), Breeze (BR), Biscem (BI), Set (SE), and Clearfil SA luting (CL). The specimens were grouped according to conditioning as follows: Group 1, polishing with 600 grit polishing paper; Group 2, silica coating with 110 microm Al2O3 particles which modified with silica; and, Group 3, tribochemical treatment--silica coating + silanization. Specimens were stored in distilled water at 37 degrees C for 24 hours before testing shear bond strength.
Silica coating and tribochemical treatment significantly increased the bond strength of the MA, UN, BR, BI, SE and CL to zirconia compared to #600 polishing. For both #600 polished and silica coating treatments, MDP-containing self-adhesive resin cement CL had the highest bond strengths to zirconia.
Applying silica coating and tribochemical treatment improved the bond strength of self-adhesive resin cement to zirconia, especially for CL.
评估不同自粘结树脂水门汀和化学机械处理对氧化锆粘结强度的交互作用。
评估了用于粘结两个氧化锆块的以下自粘结树脂水门汀:Maxcem(MA)、Smartcem(SM)、Rely X Unicem Aplicap(UN)、Breeze(BR)、Biscem(BI)、Set(SE)和 Clearfil SA 水门汀(CL)。根据以下条件对样本进行分组:第 1 组,用 600 目砂纸抛光;第 2 组,用 110 微米 Al2O3 颗粒进行硅烷化处理;第 3 组,化学机械处理——硅烷化处理+硅烷化处理。将样本在 37°C 蒸馏水中储存 24 小时,然后测试剪切粘结强度。
与 600 目抛光相比,硅烷化处理和化学机械处理显著提高了 MA、UN、BR、BI、SE 和 CL 对氧化锆的粘结强度。对于 600 目抛光和硅烷化处理,含 MDP 的自粘结树脂水门汀 CL 对氧化锆的粘结强度最高。
应用硅烷化处理和化学机械处理提高了自粘结树脂水门汀对氧化锆的粘结强度,特别是对 CL。