采用锂硅玻璃陶瓷和聚醚醚酮材料制作的嵌体的适合性和边缘间隙的比较评估——一项体外研究。

Comparative evaluation of internal fit and marginal gap of endocrowns using lithium disilicate and polyether ether ketone materials - an in vitro study.

机构信息

Bonn University, Bonn, Germany.

Faculty of Dentistry, Galala University, Suez, Egypt.

出版信息

BMC Oral Health. 2023 Apr 7;23(1):207. doi: 10.1186/s12903-023-02857-8.

Abstract

BACKGROUND

The aim of the study was to investigate the effect of material and occlusal preparation design on the internal fit and marginal gap of endocrowns made of Polyether ether ketone (PEEK) and lithium disilicate.

METHODS

32 endocrowns were fabricated on prepared mandibular molars and divided into two groups (n = 16) according to the material. Group L: lithium disilicate and Group P: PEEK. Each group was further subdivided into two subgroups (n = 8) according to the occlusal preparation design: full occlusal coverage (LF and PF) and partial occlusal coverage (LP and PP). Samples were analyzed using microcomputed tomography (µCT) with a voxel size of 6 μm to evaluate internal fit, and an optical microscope was used to evaluate the marginal gap. Data were collected, tabulated, and statistically analyzed. Numerical data were described as mean and standard deviation and compared using the ANOVA test. The level of significance was set at α P ≤ 0.05.

RESULTS

All groups' internal fit and marginal gaps values were within the acceptable clinical range. However, the lithium disilicates group recorded statistically significantly higher mean internal gap values than the PEEK groups. Regardless of the material, the difference between the two occlusal designs was not statistically significant in both internal fit and marginal gap records.

CONCLUSION

Within the limitations of this study, PEEK endocrown restorations revealed better internal fit and marginal gap than lithium disilicate endocrown restorations. The marginal and internal fit of both lithium disilicate and PEEK endocrown restorations were within the clinically acceptable range. The occlusal preparation design had no influence on the internal fit and marginal gap of the endocrown restoration.

摘要

背景

本研究旨在探讨不同材料和牙合面预备设计对内聚瓷全冠(PEEK)和锂硅瓷内冠的内部适合性和边缘间隙的影响。

方法

在预备的下颌磨牙上制作了 32 个内冠,并根据材料将其分为两组(n=16):组 L:锂硅瓷,组 P:PEEK。每组根据牙合面预备设计进一步分为两组(n=8):全牙合覆盖(LF 和 PF)和部分牙合覆盖(LP 和 PP)。使用体素大小为 6μm 的微计算机断层扫描(µCT)分析样本,以评估内部适合性,并使用光学显微镜评估边缘间隙。收集、制表和统计分析数据。数值数据以平均值和标准差表示,并使用 ANOVA 检验进行比较。显著性水平设为α P≤0.05。

结果

所有组的内部适合性和边缘间隙值均在可接受的临床范围内。然而,锂硅瓷组的内部间隙平均值记录显著高于 PEEK 组。无论材料如何,两种牙合面设计在内部适合性和边缘间隙记录方面的差异均无统计学意义。

结论

在本研究的限制范围内,PEEK 内冠修复体的内部适合性和边缘间隙优于锂硅瓷内冠修复体。锂硅瓷和 PEEK 内冠修复体的边缘和内部适合性均在临床可接受范围内。牙合面预备设计对内冠修复体的内部适合性和边缘间隙没有影响。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/4395/10082505/51fcb66de343/12903_2023_2857_Fig1_HTML.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验