Department of Radiology, Nara Medical University, Kashihara, Nara, Japan.
Cardiovasc Intervent Radiol. 2011 Jun;34(3):601-8. doi: 10.1007/s00270-010-0045-2. Epub 2010 Dec 10.
This study was designed to clarify the advantages of biodegradable stents in terms of mucosal reaction and biodegradation after placement. We designed a biodegradable stent and assessed stent degradation and changes in the normal bile ducts of dogs.
The biodegradable stent is a balloon-expandable Z stent consisting of poly-L-lactic acid (PLLA) with a diameter of 6 mm and a length of 15 mm. We assessed four groups of three beagle dogs each at 1, 3, 6, and 9 months of follow-up. After evaluating stent migration by radiography and stent and bile duct patency by cholangiography, the dogs were sacrificed to remove the bile duct together with the stent. The bile duct lumen was examined macroscopically and histologically, and the stent degradation was examined macroscopically and by scanning electron microscopy (SEM).
Bile duct obstruction was absent and none of the stents migrated. Macroscopic evaluation showed moderate endothelial proliferation in the bile ducts at the implant sites at 3 and 6 months and a slight change at 9 months. Slight mononuclear cell infiltration was histologically identified at all time points and epithelial hyperplasia that was moderate at 3 months was reduced to slight at 6 and 9 months. Stent degradation was macroscopically evident in all animals at 9 months and was proven by SEM in two dogs at 6 months and in all of them at 9 months.
Our results suggest that PLLA bioabsorbable stents seems to be useful for implantation in the biliary system with further investigation.
本研究旨在阐明可生物降解支架在放置后黏膜反应和生物降解方面的优势。我们设计了一种可生物降解支架,并评估了支架的降解和犬正常胆管的变化。
可生物降解支架是一种球囊扩张 Z 支架,由聚 L-乳酸(PLLA)制成,直径 6mm,长 15mm。我们在 1、3、6 和 9 个月的随访中评估了每组 3 只比格犬的 4 个组。通过 X 线摄影评估支架迁移情况,通过胆管造影评估支架和胆管通畅情况后,将犬处死并取出胆管和支架。检查胆管管腔的大体和组织学变化,并通过扫描电子显微镜(SEM)检查支架降解情况。
无胆管阻塞,无支架迁移。大体评估显示,在植入部位的胆管中,3 个月和 6 个月时内皮细胞中度增生,9 个月时略有变化。所有时间点均有轻度单核细胞浸润,3 个月时上皮细胞增生中度,6 个月和 9 个月时减少为轻度。所有动物在 9 个月时均在大体上可见支架降解,在 6 个月时有 2 只犬通过 SEM 证实,在 9 个月时有所有犬证实。
我们的结果表明,PLLA 可生物吸收支架似乎可用于胆道植入,进一步的研究是必要的。