Division of Dental Biomaterials, Department of Restorative Dentistry, Indiana University School of Dentistry, Indianapolis, IN 46202, USA.
Int Endod J. 2013 Feb;46(2):112-8. doi: 10.1111/j.1365-2591.2012.02121.x. Epub 2012 Sep 13.
The aim of this review was to identify and analyse all studies related to the effect of nonsetting calcium hydroxide [Ca(OH)(2)] on root fracture and various mechanical properties of radicular dentine. A PubMed search was conducted using the keywords 'calcium hydroxide' and 'dentistry' combined with MeSH terms 'tooth fractures' or 'mechanical phenomena' or 'compressive strength'. The search was expanded by including Embase and Web of Science databases, using the keywords 'calcium hydroxide' and 'root' and 'fracture'. The search was supplemented by checking the reference lists from each selected article. Each study had to meet the following criteria to be selected for review: (i) Inclusion of at least one experimental group with root or radicular dentine either filled with or exposed to nonsetting Ca(OH)(2); (ii) inclusion of at least one appropriate control group; and (iii) a minimum of five samples per experimental group. Only articles written in English were included. Of the 16 studies selected initially, 12 in vitro studies fulfilled the selection criteria for inclusion in the final review. No clinical studies that directly supported the correlation between Ca(OH)(2) intracanal dressing and root fracture were found in the literature. However, the majority of in vitro studies showed reduction in the mechanical properties of radicular dentine after exposure to Ca(OH)(2) for 5 weeks or longer. Conversely, the data were inconclusive regarding whether Ca(OH)(2) exposure for 1 month or less had a negative effect on the mechanical properties of radicular dentine.
本综述的目的是识别和分析所有与非凝固氢氧化钙(Ca(OH)(2))对牙根折断和根管牙本质各种力学性能的影响相关的研究。使用关键词“氢氧化钙”和“牙科学”,并结合 MeSH 术语“牙折”或“力学现象”或“抗压强度”,在 PubMed 上进行了检索。通过包括 Embase 和 Web of Science 数据库,使用关键词“氢氧化钙”和“根”和“断裂”,对搜索进行了扩展。通过检查每个选定文章的参考文献列表,对搜索进行了补充。为了被选为综述,每一项研究都必须符合以下标准:(i) 至少有一个实验组,其根管或根管牙本质填充或暴露于非凝固 Ca(OH)(2);(ii) 至少有一个合适的对照组;和 (iii) 每个实验组至少有五个样本。仅包括用英语撰写的文章。在最初选择的 16 项研究中,有 12 项体外研究符合纳入最终综述的选择标准。文献中没有直接支持 Ca(OH)(2)根管内封药与牙根折断之间相关性的临床研究。然而,大多数体外研究表明,暴露于 Ca(OH)(2) 5 周或更长时间后,根管牙本质的力学性能会降低。相反,关于暴露于 Ca(OH)(2) 1 个月或更短时间是否会对根管牙本质的力学性能产生负面影响,数据尚无定论。