School of Chemistry and Chemical Engineering, Anhui University, Hefei 230039, PR China.
J Phys Chem B. 2013 Apr 11;117(14):3720-5. doi: 10.1021/jp3110908. Epub 2013 Apr 3.
Superparamagnetic Fe3O4 nanoparticles were obtained using a hydrolysis product of starch, i.e., α-d-glucose, as the reducing agent and without any additional stabilizer and dispersant by a facile and green method at mild temperature. Magnetic dialdehyde starch nanoparticles (MDASN) were successfully synthesized with dialdehyde starch (DAS) as wrapper and epichlorohydrin as cross-linker by coembedding method. Bovine serum albumin (BSA) as a model drug was immobilized on the suface of MDASN. The particle size distribution of MDASN was 50-150 nm, and the average size was about 100 nm. The content of aldehyde group in DAS was 59.5%, and the package rate of DAS in MDASN was 33.2%. The loading amount and encapsulation efficiency of MDASN loading BSA were 5.0% and 54.4%, respectively. The saturation magnetization of MDASN at 300 K was 29.5 emu/g without coercivity and remanence. The as-prepared MDASN have not only lots of aldehyde functional groups but also stronger magnetic response, which might have potential applications such as drug carriers and targeted drug release.
采用淀粉的水解产物α-d-葡萄糖作为还原剂,在温和的温度下通过简便、绿色的方法,无需添加任何额外的稳定剂和分散剂,成功制备了超顺磁四氧化三铁纳米粒子。以双醛淀粉(DAS)为包裹剂,以环氧氯丙烷为交联剂,采用共嵌入法成功合成了磁性二醛淀粉纳米粒子(MDASN)。将牛血清白蛋白(BSA)作为模型药物固定在 MDASN 的表面。MDASN 的粒径分布为 50-150nm,平均粒径约为 100nm。DAS 中的醛基含量为 59.5%,DAS 在 MDASN 中的包封率为 33.2%。MDASN 负载 BSA 的载药量和包封率分别为 5.0%和 54.4%。在 300K 时,MDASN 的饱和磁化强度为 29.5emu/g,无矫顽力和剩磁。所制备的 MDASN 不仅具有大量的醛基官能团,而且具有更强的磁响应,可能在药物载体和靶向药物释放等方面具有潜在的应用。