Weissheimer André, Locks Arno, de Menezes Luciane Macedo, Borgatto Adriano Ferreti, Derech Carla D'Agostini
PUC-RS.
Dental Press J Orthod. 2013 Jan-Feb;18(1):55-62. doi: 10.1590/s2176-94512013000100014.
To analyze the in vitro force degradation of four different brands of elastomeric chains: American Orthodontics, Morelli, Ormco and TP Orthodontics.
The sample consisted of 80 gray elastomeric chains that were divided into four groups according to their respective manufacturers. Chain stretching was standardized at 21 mm with initial force release ranging from 300 g to 370 g. The samples were kept in artificial saliva at a constant temperature of 37°C and the degradation force was recorded at the following time intervals: initial, 1, 3, 5, 7 and 9 hours, and 1, 7, 14, 21, 28, and 35 days.
There was a statistically significant difference between the groups regarding the force degradation, mainly within the first day, as a force loss of 50-55% was observed during that time in relation to the initial force. The force delivered at 35 days ranged from 122 g to 148 g.
All groups showed force degradation over time, regardless of their trademarks, a force loss of 59-69% was observed in the first hour compared to baseline. However, because the variation in force degradation depends on the trademark, studies such as the present one are important for guiding the clinical use of these materials.
分析四种不同品牌(美国正畸、莫雷利、奥美科和TP正畸)的弹性链在体外的力降解情况。
样本由80条灰色弹性链组成,根据各自制造商分为四组。链拉伸标准化为21毫米,初始力释放范围为300克至370克。样本置于37°C恒温的人工唾液中,并在以下时间间隔记录降解力:初始、1、3、5、7和9小时,以及1、7、14、21、28和35天。
各小组在力降解方面存在统计学上的显著差异,主要在第一天内,此时相对于初始力观察到力损失50 - 55%。35天时施加的力范围为122克至148克。
所有组均显示随着时间的推移力发生降解,无论其商标如何,与基线相比,在第一小时观察到力损失59 - 69%。然而,由于力降解的变化取决于商标,像本研究这样的研究对于指导这些材料的临床应用很重要。