Maghaireh Ghada A, Alzraikat Hanan, Taha Nessrin A
Department of Conservative Dentistry, Jordan University of Science and Technology, P.O. Box 3030, Irbid-22110, Jordan.
J Am Dent Assoc. 2013 Aug;144(8):922-7. doi: 10.14219/jada.archive.2013.0210.
The authors conducted a study to examine the irradiance from light-curing units (LCUs) used in dental offices in Jordan.
Two of the authors visited 295 private dental offices (15 percent) in Jordan and collected the following information about the LCUs: age, type (quartz-tungsten-halogen or light-emitting diode), date of last maintenance, type of maintenance, last date of use, number of times used during the day, availability of a radiometer, exposure time for each resin-based composite increment, size of light-curing tips and presence of resin-based composite on the tips. The authors used a radiometer to measure the irradiance from the LCUs. They used linear regression with stepwise correlation for the statistical analysis. The authors set the minimum acceptable irradiance at 300 milliwatts/square centimeter.
The mean irradiance of the 295 LCUs examined was 361 mW/cm(2), and 136 LCUs (46.1 percent) delivered an irradiance of less than 300 mW/cm(2). The unit's age, type and presence of resin-based composite on the light-curing tips had a significant effect on the irradiance (P ≤ .001).
Only 37 of the 141 quartz-tungsten-halogen units (26.2 percent) and 122 of the 154 light-emitting diode units (79.2 percent) delivered at least 300 mW/cm(2). Resin contamination on the light-curing tips had a significant effect on the irradiance delivered. The irradiance from the LCUs decreased with use. Practical Implications. The irradiance from many of the units in this study was less than 300 mW/cm(2), which may affect the quality of resin-based composite restorations. Dentists should monitor the performance of the LCUs in their offices weekly.
作者开展了一项研究,以检测约旦牙科诊所使用的光固化机(LCU)的辐照度。
两位作者走访了约旦295家私人牙科诊所(占15%),收集了有关光固化机的以下信息:使用年限、类型(石英钨卤素灯或发光二极管)、上次维护日期、维护类型、上次使用日期、每日使用次数、是否配备辐射计、每次复合树脂增量的照射时间、光固化头尺寸以及光固化头上是否有复合树脂。作者使用辐射计测量光固化机的辐照度。他们采用逐步相关的线性回归进行统计分析。作者将可接受的最低辐照度设定为300毫瓦/平方厘米。
所检测的295台光固化机的平均辐照度为361 mW/cm²,136台光固化机(46.1%)的辐照度低于300 mW/cm²。光固化机的使用年限、类型以及光固化头上复合树脂的存在对辐照度有显著影响(P≤0.001)。
141台石英钨卤素灯中只有37台(26.2%),154台发光二极管光固化机中有122台(79.2%)的辐照度至少为300 mW/cm²。光固化头上的树脂污染对辐照度有显著影响。光固化机的辐照度随使用而降低。实际意义。本研究中许多光固化机的辐照度低于300 mW/cm²,这可能会影响复合树脂修复体的质量。牙医应每周监测其诊所内光固化机的性能。