Suppr超能文献

第一代高度交联聚乙烯在初次全髋关节置换术中的10年随访磨损分析

10-year follow-up wear analysis of first-generation highly crosslinked polyethylene in primary total hip arthroplasty.

作者信息

Snir Nimrod, Kaye Ian D, Klifto Christopher S, Hamula Mathew J, Wolfson Theodore S, Schwarzkopf Ran, Jaffe Fredrick F

机构信息

Department of Orthopaedic Surgery, New York University Hospital for Joint Diseases, New York, New York.

Department of Orthopaedic Surgery, University of California Irvine Medical Center, Orange, California.

出版信息

J Arthroplasty. 2014 Mar;29(3):630-3. doi: 10.1016/j.arth.2013.07.034. Epub 2013 Aug 29.

Abstract

Our goal was to report a 10-year follow up of linear penetration rates for HCLPE, and to determine whether a difference exists between penetrations measured on pelvis or hip anterior-posterior radiographs. We reviewed 48 total hip arthroplasties where a first-generation HCLPE liner was used. Femoral head penetration was measured on both AP pelvis and hip radiographs. Total wear and wear rate at 10 years were 1.26 mm and 0.122 mm/y, respectively. The rate decreased significantly after the first 2-3 years, plateauing at a wear rate of 0.05 mm/y for the last 5 years. The AP hip total wear and wear rate were 1.38 mm and 0.133 mm/y respectively, while rates were 1.13 mm and 0.109 mm/y respectively for the pelvis radiographs (P<.05). We found a significant difference in measurements of linear penetration when comparing AP pelvis vs. hip radiographs with lower rates recorded using an AP pelvis.

摘要

我们的目标是报告毛面髋臼内衬聚乙烯(HCLPE)线性磨损率的10年随访情况,并确定在骨盆或髋关节前后位X线片上测量的磨损率是否存在差异。我们回顾了48例使用第一代HCLPE内衬的全髋关节置换术。在骨盆前后位和髋关节前后位X线片上测量股骨头磨损情况。10年时的总磨损量和磨损率分别为1.26 mm和0.122 mm/年。在最初2至3年后磨损率显著下降,在最后5年稳定在0.05 mm/年的磨损率。髋关节前后位的总磨损量和磨损率分别为1.38 mm和0.133 mm/年,而骨盆X线片的磨损量和磨损率分别为1.13 mm和0.109 mm/年(P<0.05)。我们发现,比较骨盆前后位与髋关节前后位X线片时,线性磨损测量存在显著差异,使用骨盆前后位X线片记录的磨损率较低。