丁香酚暴露时间对两步法和一步法自酸蚀粘结剂与牙本质剪切粘结强度影响的体外评估

An in vitro evaluation of effect of eugenol exposure time on the shear bond strength of two-step and one-step self-etching adhesives to dentin.

作者信息

Nasreen Farhat, Guptha Anila Bandlapalli Sreenivasa, Srinivasan Raghu, Chandrappa Mahesh Martur, Bhandary Shreetha, Junjanna Pramod

机构信息

Department of Conservative Dentistry and Endodontics, Amrith Educational and Cultural Society Maaruti College of Dental Sciences and Research Centre, Bangalore, Karnataka, India.

出版信息

J Conserv Dent. 2014 May;17(3):280-4. doi: 10.4103/0972-0707.131802.

Abstract

OBJECTIVES

To evaluate the effect of the eugenol exposure time of an eugenol-based provisional restorative material on the shear bond strength of two-step and one-step self-etching adhesives to dentin, at three different time intervals of 24 h, 7 days, and 14 days.

MATERIALS AND METHODS

Forty extracted human posterior teeth were sectioned mesiodistally to obtain two halves and the resulting 80 halves were randomly assigned into four groups of 20 specimens each (Group-I, -II, -III, and -IV). Cavities of specified dimensions were prepared to expose dentin surface. In Group-I, temporarization was carried out with noneugenol cement (Orafil-G) for 24 h (control group). In Group-II, -III, and -IV, temporarization was carried out with eugenol cement (intermediate restorative material (IRM)) for 24 h, 7 days, and 14 days, respectively. Each group was further divided into two subgroups of 10 teeth each for two-step (Adper SE Plus) and one-step (Adper Easy One) self-etch adhesive systems, respectively. A plastic tube loaded with microhybrid composite resin (Filtek Z-350, 3M) was placed over the dentin surface and light cured. The specimens were subjected to shear stress in universal testing machine.

RESULTS

Group-II yielded low shear bond strength values compared with Group-III, -IV, and Group-I, which was statistically significant.

CONCLUSIONS

The prior use of eugenol containing temporary restorative material reduced the bond strength of self-etch adhesive systems at 24-h period. No reduction in bond strength at 7 or 14 days exposure was observed with either two-step or one-step self-etch adhesive.

摘要

目的

评估一种含丁香酚的临时修复材料的丁香酚暴露时间,对两种两步法和一步法自酸蚀粘结剂在牙本质上的剪切粘结强度的影响,时间间隔为24小时、7天和14天这三个不同时间段。

材料与方法

40颗拔除的人类后牙沿近远中方向切片,得到两半,共80个半片随机分为四组,每组20个样本(第一组、第二组、第三组和第四组)。制备特定尺寸的窝洞以暴露牙本质表面。在第一组中,用不含丁香酚的水门汀(Orafil-G)进行临时修复24小时(对照组)。在第二组、第三组和第四组中,分别用含丁香酚的水门汀(中间修复材料(IRM))进行临时修复24小时、7天和14天。每组再进一步分为两个亚组,每组10颗牙,分别用于两步法(Adper SE Plus)和一步法(Adper Easy One)自酸蚀粘结剂系统。将装有微混合复合树脂(Filtek Z-350,3M)的塑料管置于牙本质表面并光固化。在万能试验机上对样本施加剪切应力。

结果

与第三组、第四组和第一组相比,第二组的剪切粘结强度值较低,具有统计学意义。

结论

预先使用含丁香酚的临时修复材料在24小时内降低了自酸蚀粘结剂系统的粘结强度。对于两步法或一步法自酸蚀粘结剂,在暴露7天或14天时未观察到粘结强度降低。