Goswami Arunima, Mitali Borah, Roy Bk
Department of Orthodontics and Dentofacial Orthopaedics, Regional Dental College, Guwahati, Assam, India.
J Orthod Sci. 2014 Jul;3(3):89-93. doi: 10.4103/2278-0203.137695.
The detrimental effect of moisture on orthodontic bonding has long been known. Hydrophilic bonding materials have been introduced suggesting the possibility of obtaining successful orthodontic bonding to a moisture contaminated enamel surface.
This study has been performed with an aim to compare the in vitro shear bond strength (SBS) and debonding characteristic of moisture-insensitive primer (MIP) (Transbond MIP) (3M Unitek, South Peck Road, Monrovia, California, USA) and self-etching primer (SEP) (Transbond Plus SEP) (3M Unitek, South Peck Road, Monrovia, California, USA) in combination with a color changing adhesive system (Transbond Plus Color Change) (3M Unitek, South Peck Road, Monrovia, California, USA) under both dry and contaminated condition.
Randomized controlled clinical study.
One hundred and twenty freshly extracted teeth for the purpose of orthodontic treatment were collected. Teeth were randomly assigned into four groups, each consisting of 30 specimen and stainless steel brackets were bonded using each primer-adhesive combination under different enamel conditions, that is, dry and enamel contaminated with natural saliva. SBS and adhesive remnant index were calculated for each group.
Analysis of variance of SBS for both MIP and SEP under dry and contaminated condition showed no statistical significance (P = 0.5). Chi-square test showed significant difference in debonding characteristics among the test groups (P < 0.001). All the groups showed typical debonding characteristics of separation either at the bracket-adhesive interface or within the adhesive itself.
Moisture contamination did not affect the SBS and adhesive remaining on tooth for both MIP and SEP.
长期以来,人们一直知道水分对正畸粘结有不利影响。引入了亲水性粘结材料,这表明有可能在被水分污染的牙釉质表面成功进行正畸粘结。
本研究旨在比较在干燥和污染条件下,水分不敏感底漆(MIP)(Transbond MIP)(美国加利福尼亚州蒙罗维亚南佩克路3M Unitek公司)和自酸蚀底漆(SEP)(Transbond Plus SEP)(美国加利福尼亚州蒙罗维亚南佩克路3M Unitek公司)与变色粘结系统(Transbond Plus Color Change)(美国加利福尼亚州蒙罗维亚南佩克路3M Unitek公司)联合使用时的体外剪切粘结强度(SBS)和脱粘特性。
随机对照临床研究。
收集120颗用于正畸治疗的新鲜拔除牙齿。将牙齿随机分为四组,每组30个样本,并在不同的牙釉质条件下,即干燥和被天然唾液污染的牙釉质上,使用每种底漆 - 粘结剂组合粘结不锈钢托槽。计算每组的SBS和粘结剂残留指数。
在干燥和污染条件下,MIP和SEP的SBS方差分析显示无统计学意义(P = 0.5)。卡方检验显示试验组之间的脱粘特性有显著差异(P < 0.001)。所有组在托槽 - 粘结剂界面或粘结剂内部均表现出典型的分离脱粘特性。
水分污染对MIP和SEP的SBS以及牙齿上残留的粘结剂均无影响。