Dewo P, van der Houwen E B, Marius R, Magetsari R, Verkerke G J
Department of Orthopaedics and Traumatology Sardjito Hospital/Universitas Gadjah Mada, Yogyakarta, Indonesia.
Department of Industrial Design, Eindhoven University of Technology, Eindhoven, the Netherlands.
J Mech Behav Biomed Mater. 2015 Feb;42:274-81. doi: 10.1016/j.jmbbm.2014.11.025. Epub 2014 Dec 1.
Mechanical properties determined by fatigue strength, ductility, and toughness are important measures for osteosynthesis plates in order to tolerate some load-bearing situations caused by muscle contractions and weight-bearing effects. Previous study indicated that Indonesian-made plates showed lower mechanical strength compared to the European AO standard plate. High stress under load-bearing situations often starts from surface of the plate; we therefore refined the grain size of the surface by using shot peening and surface mechanical attrition treatment (SMAT). Single cycle bending tests showed that shot-peened and SMAT-treated plates had significantly higher load limit and bending stress compared to the original plates (p<0.05). Weibull analysis confirmed the improvement of proportional load limit of SMAT-treated plates. Fatigue limit also increased upon shot-peening and SMAT treatment (improvement ratio 18% and 27%, respectively). Significant improvement ratio of fatigue tests can be observed in SMAT-treated plates compared to the untreated and shot-peened plates. Fatigue performance demonstrated equivalent results between SMAT-treated and standard plate. These designated that mechanical properties of Indonesian-made plates can be improved upon SMAT treatment leading to significant enhancement of mechanical strength thus is comparable to the standard plate. Our findings highlight the benefits of SMAT treatment to improve mechanical strength of Indonesian-made osteosynthesis plates.
由疲劳强度、延展性和韧性所决定的机械性能是接骨板的重要指标,以便承受由肌肉收缩和负重效应引起的一些承重情况。先前的研究表明,与欧洲AO标准接骨板相比,印度尼西亚制造的接骨板机械强度较低。承重情况下的高应力通常从接骨板表面开始;因此,我们通过喷丸处理和表面机械研磨处理(SMAT)细化了表面晶粒尺寸。单循环弯曲试验表明,与原始接骨板相比,喷丸处理和SMAT处理的接骨板具有显著更高的负载极限和弯曲应力(p<0.05)。威布尔分析证实了SMAT处理的接骨板比例负载极限有所提高。喷丸处理和SMAT处理后疲劳极限也有所增加(提高率分别为18%和27%)。与未处理和喷丸处理的接骨板相比,SMAT处理的接骨板在疲劳试验中可观察到显著的提高率。疲劳性能在SMAT处理的接骨板和标准接骨板之间表现出等效结果。这些表明,印度尼西亚制造的接骨板经SMAT处理后机械性能可以得到改善,从而显著提高机械强度,与标准接骨板相当。我们的研究结果突出了SMAT处理对提高印度尼西亚制造的接骨板机械强度的益处。