Mater Sci Eng C Mater Biol Appl. 2015 Mar;48:256-62. doi: 10.1016/j.msec.2014.12.011. Epub 2014 Dec 6.
This study aimed to evaluate the cytocompatibility and early osseointegration of Ti-24 Nb-4 Zr-7.9 Sn (Ti-2448) surfaces that were modified with a nanoscale TiO2 coating. The coating was fabricated using a hydrothermal synthesis method to generate nanoTiO2/Ti-2448. The surface characteristics of the samples were evaluated using scanning electron microscopy (SEM), energy dispersive spectrometry (EDS) and X-ray diffraction (XRD). The cytotoxicity of the fabricated nanoTiO2/Ti-2448 was determined using MTT assays. The proliferation and alkaline phosphatase (ALP) activity of MC3T3-E1 osteoblasts cultured on nanoTiO2/Ti-2448 were compared with those cultured on Ti-2448. Disk-shaped implants were placed in Wistar rats. The histological sections were stained with haematoxylin and eosin (HE), and the histocompatibility was analysed at 4 and 12weeks post-implantation. Cylindrical implants were embedded in Japanese white rabbits, and the histological sections were stained with HE and anti-TGF-β1 to evaluate the histocompatibility and early osseointegration at 4, 12 and 26weeks post-implantation. NanoTiO2/Ti-2448 exhibited a rougher surface than did Ti-2448. NanoTiO2/Ti-2448 was determined to be non-cytotoxic. More osteoblasts and higher ALP activity were observed for nanoTiO2/Ti-2448 than Ti-2448 (p<0.05). Few inflammatory cells were detected around nanoTiO2/Ti-2448, and the expression of TGF-β1 on nanoTiO2/Ti-2448 peaked at earlier time than that on Ti-2448. The results indicate that the cytocompatibility and early osseointegration were enhanced by the nanoTiO2 coating.
本研究旨在评估经过纳米 TiO2 涂层改性的 Ti-24 Nb-4 Zr-7.9 Sn(Ti-2448)表面的细胞相容性和早期骨整合。该涂层采用水热合成法制备,生成纳米 TiO2/Ti-2448。采用扫描电子显微镜(SEM)、能谱仪(EDS)和 X 射线衍射(XRD)对样品表面特性进行评估。采用 MTT 法测定制备的纳米 TiO2/Ti-2448 的细胞毒性。比较了纳米 TiO2/Ti-2448 上培养的 MC3T3-E1 成骨细胞的增殖和碱性磷酸酶(ALP)活性与 Ti-2448 上培养的细胞。将盘状植入物放置在 Wistar 大鼠体内。用苏木精和伊红(HE)染色组织切片,分析植入后 4 和 12 周的组织相容性。将圆柱形植入物嵌入日本白兔体内,用 HE 和抗 TGF-β1 染色组织切片,评估植入后 4、12 和 26 周的组织相容性和早期骨整合。与 Ti-2448 相比,纳米 TiO2/Ti-2448 具有更粗糙的表面。纳米 TiO2/Ti-2448 被确定为非细胞毒性。与 Ti-2448 相比,纳米 TiO2/Ti-2448 观察到更多的成骨细胞和更高的 ALP 活性(p<0.05)。在纳米 TiO2/Ti-2448 周围检测到很少的炎症细胞,并且纳米 TiO2/Ti-2448 上 TGF-β1 的表达早于 Ti-2448 上的表达。结果表明,纳米 TiO2 涂层增强了细胞相容性和早期骨整合。