Eliche-Quesada D, Leite-Costa J
Department of Chemical, Environmental, and Materials Engineering, Higher Polytechnic School of Jaén, University of Jaen, Campus Las Lagunillas s/n, 23071 Jaén, Spain.
Department of Chemical, Environmental, and Materials Engineering, Higher Polytechnic School of Linares, University of Jaen, 23700 Linares (Jaen), Spain.
Waste Manag. 2016 Feb;48:323-333. doi: 10.1016/j.wasman.2015.11.042. Epub 2015 Dec 2.
Olive pomace bottom ash was used to replace different amounts (10-50wt%) of clay in brick manufacturing. The aim of this study is both studying bricks properties and showing a new way of olive pomace bottom ash recycling. Properties of waste bricks were compared to conventional products following standard procedures in order to determine the maximum waste percentage. The amount of olive pomace bottom ash is limited to 20wt%, obtaining bricks with superior engineering properties when 10wt% of waste is added. Adding higher amount of waste (30-50wt%) resulted in bricks with water absorption and compressive strength values on the edge of meeting those established by standards. Therefore, the addition of 10 and 20wt% of olive pomace bottom ash produced bricks with a bulk density of 1635 and 1527kg/m(3) and a compressive strength of 33.9MPa and 14.2MPa, respectively. Fired bricks fulfil standards requirements for clay masonry units, offering, at the same time, better thermal insulation of buildings due to a reduction in thermal conductivity of 14.4% and 16.8% respectively, compared to control bricks (only clay).
橄榄果渣底灰被用于在制砖过程中替代不同比例(10 - 50重量%)的黏土。本研究的目的是研究砖块性能并展示橄榄果渣底灰回收利用的新方法。按照标准程序,将废弃砖块的性能与传统产品进行比较,以确定最大废料百分比。橄榄果渣底灰的用量限制在20重量%,当添加10重量%的废料时,可得到具有优异工程性能的砖块。添加更高比例的废料(30 - 50重量%)会导致砖块的吸水率和抗压强度值接近但未达到标准规定值。因此,添加10重量%和20重量%的橄榄果渣底灰分别制得的砖块,其堆积密度为1635和1527kg/m³,抗压强度分别为33.9MPa和14.2MPa。烧制砖符合黏土砌体单元的标准要求,同时,与对照砖(仅含黏土)相比,由于导热系数分别降低了14.4%和16.8%,可为建筑物提供更好的隔热性能。