Suppr超能文献

功能性磷酸酯单体在氧化钇稳定四方多晶氧化锆表面处理中的作用。

The role of functional phosphoric acid ester monomers in the surface treatment of yttria-stabilized tetragonal zirconia polycrystals.

作者信息

Arai Masami, Takagaki Tomohiro, Takahashi Akifumi, Tagami Junji

机构信息

Cariology and Operative Dentistry, Department of Oral Health Sciences, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University.

出版信息

Dent Mater J. 2017 Mar 31;36(2):190-194. doi: 10.4012/dmj.2016-060. Epub 2017 Jan 20.

Abstract

This study aimed to evaluate the bond strength of a resin cement to yttria-stabilized tetragonal zirconia polycrystals (Y-TZPs) treated with three different phosphate functional monomers containing primers by measuring the water contact angle. Seventy Y-TZP discs were divided into seven experimental groups (n=10), including an untreated (control) group. Specimens were treated with one of the following monomers: MDP (MD), GPDM (GP), and Phenyl-P (PP). After primer application and air drying, half the treated specimens were ultrasonically cleaned in ethanol for 2 min (MD-e, GP-e, and PP-e), and contact angles were measured. The tensile bond strength test was performed after storage for 24 h in 37°C water. The contact angle on the MD-e surface (64°) was significantly higher than that on the Con, GP-e, and PP-e surfaces (51°-52°). The application of the MDP-containing primer resulted in significantly higher bond strength between Y-TZP ceramics and a resin cement.

摘要

本研究旨在通过测量水接触角来评估一种树脂水门汀与经三种不同含磷酸酯功能单体的底漆处理的氧化钇稳定四方多晶氧化锆(Y-TZP)之间的粘结强度。将70个Y-TZP圆盘分为7个实验组(n = 10),包括一个未处理(对照)组。用以下单体之一处理试样:10-甲基丙烯酰氧癸基二氢磷酸酯(MD)、甘油磷酸甲基丙烯酸酯(GP)和苯基膦酸(PP)。涂覆底漆并空气干燥后, 一半处理过的试样在乙醇中超声清洗2分钟(MD-e、GP-e和PP-e),并测量接触角。在37°C水中储存24小时后进行拉伸粘结强度测试。MD-e表面的接触角(64°)显著高于对照组、GP-e和PP-e表面的接触角(51°- 52°)。含MD底漆的应用导致Y-TZP陶瓷与树脂水门汀之间的粘结强度显著更高。