Polymers (Basel). 2017 Jul 20;9(7):289. doi: 10.3390/polym9070289.
This study developed the interests of low-methoxyl pectin (LMP) together with plasticizers for the preparation of elastic thin films. The effect of different plasticizer types (glycerol: Gly; sorbitol: Sor; propylene glycol: PG; and polyethylene glycol 300: PEG 300) and concentrations (20⁻40% ) on mechanical and thermal properties of LMP films as well as on in vitro release of indomethacin were evaluated. Without any plasticizer, a brittle LMP film with low tensile strength and % elongation at break was obtained. Addition of plasticizers from 20% to 40% caused reduction in the tensile strength and Young's modulus values, whereas percent elongation was increased. Forty percent Gly-plasticized and PG-plasticized films were selected to deliver indomethacin in comparison with non-plasticized film. No significant difference in indomethacin release profiles was displayed between the films. The analysis of indomethacin release model indicated that more than one drug release mechanism from the film formulation was involved and possibly the combination of both diffusion and erosion. Even though indomethacin incorporated in non-plasticized film showed similar release profile, Gly or PG should be added to enhanced film flexibility and decrease film brittleness.
本研究开发了低甲氧基果胶(LMP)与增塑剂用于制备弹性薄膜。评估了不同类型增塑剂(甘油:Gly;山梨醇:Sor;丙二醇:PG;聚乙二醇300:PEG 300)及其浓度(20⁻40%)对LMP薄膜力学性能、热性能以及吲哚美辛体外释放的影响。未添加任何增塑剂时,得到了一种拉伸强度和断裂伸长率较低的脆性LMP薄膜。添加20%至40%的增塑剂会导致拉伸强度和杨氏模量值降低,而断裂伸长率增加。选择40%甘油增塑和丙二醇增塑的薄膜与未增塑薄膜相比用于递送吲哚美辛。各薄膜之间吲哚美辛释放曲线无显著差异。吲哚美辛释放模型分析表明,薄膜制剂中涉及不止一种药物释放机制,可能是扩散和溶蚀的组合。尽管未增塑薄膜中掺入的吲哚美辛显示出相似的释放曲线,但应添加甘油或丙二醇以提高薄膜柔韧性并降低薄膜脆性。