Abstract

BACKGROUND

Orthodontic bonding and debonding procedures involve risk of damaging the enamel surface and changing its original morphology. The rough surface inhibits proper cleaning, invites plaque deposition, bacterial retention, and stain formation thus dampening the esthetic appearance of the teeth. Restoring the enamel to its original morphology is a challenge. Researches on better adhesive removal methods which can effectively remove the residual resin and restore it best to its original form are continuing till date. No study has compared four contemporary finishing systems for their efficiency on a single platform.

AIM

The objective of this study is to evaluate and compare enamel surface roughness after debonding using four different finishing and polishing systems.

MATERIAL AND METHODS

Adhesive resin was removed from the buccal surface of 88 premolars after debonding with 4 groups. It included 22 teeth per group: group 1-One gloss system; group 2-Enhance finishing and polishing system; group 3-fiber reinforced stainbuster bur; and group 4-Soflex discs with wheels. Roughness was measured quantitatively and qualitatively with the help of surface roughness tester and scanning electron Microscope (SEM) respectively.

RESULTS

No significant difference was found in baseline roughness in four groups. Highest post-polishing roughness was observed in Soflex group (4.62 μm) followed by One gloss system (3.36 μm), Enhance system (3.17 μm), and stainbuster bur (1.99 μm) (p value < 0.01).

CONCLUSION

Stainbuster bur created the smoothest enamel surface that was close to the natural enamel followed by Enhance system, One gloss system, and Soflex disc and wheels.

摘要

背景

正畸粘接和脱粘程序涉及到损害釉质表面并改变其原始形态的风险。粗糙的表面妨碍了适当的清洁,容易导致牙菌斑沉积、细菌滞留和污渍形成,从而降低了牙齿的美观度。恢复釉质的原始形态是一个挑战。目前仍在研究更好的去除黏合剂的方法,这些方法可以有效地去除残留的树脂,并使其尽可能恢复到原来的形态。迄今为止,还没有研究比较过四种当代的修整系统在单一平台上的效率。

目的

本研究旨在评估和比较使用四种不同的修整和抛光系统在脱粘后对釉质表面粗糙度的影响。

材料和方法

在脱粘后,用 4 组分别从 88 颗前磨牙的颊面去除黏附树脂。每组包括 22 颗牙齿:第 1 组-One gloss 系统;第 2 组-Enhance 修整和抛光系统;第 3 组-纤维增强染色抑制剂磨头;第 4 组-Soflex 盘和车轮。使用表面粗糙度测试仪和扫描电子显微镜(SEM)分别对粗糙度进行定量和定性测量。

结果

在 4 组中,基线粗糙度没有显著差异。Soflex 组的后抛光粗糙度最高(4.62 μm),其次是 One gloss 系统(3.36 μm)、Enhance 系统(3.17 μm)和染色抑制剂磨头(1.99 μm)(p 值<0.01)。

结论

染色抑制剂磨头所产生的釉质表面最光滑,接近天然釉质,其次是 Enhance 系统、One gloss 系统和 Soflex 盘和车轮。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/ad18/6500785/2b8398069786/40510_2019_269_Fig1_HTML.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验