Suppr超能文献

高粱秸秆:制浆和漂白工艺优化及醋酸纤维素的合成。

Sorghum straw: Pulping and bleaching process optimization and synthesis of cellulose acetate.

机构信息

Postgraduate of Agricultural Engineering Course, Universidade Estadual de Goiás, UEG Anápolis Campus of Exact and Technological Sciences - Henrique Santillo, BR 153 Quadra Área, Km 99, Anápolis, Goiás, Brazil.

Industrial Chemistry Course, UEG Anápolis, Brazil.

出版信息

Int J Biol Macromol. 2019 Aug 15;135:877-886. doi: 10.1016/j.ijbiomac.2019.05.014. Epub 2019 May 29.

Abstract

The process employed for the pulping and bleaching of sorghum straw was optimized prior to the synthesis of cellulose acetate. A 2 factorial central composite design was carried out. The variables considered were cooking time (1.5 to 2.5 h) and dilute alkali concentration (0.75 to 1.25%) for the pulping and bleaching time (30 to 35 min) and bleach volume (20 to 25 mL) for the bleaching. The sorghum straw was comprised of 49.43% α-cellulose, 19.18% hemicellulose and 30.42% lignin. The optimum conditions that maximize these processes were 2.5 h and 1.25% (dilute alkali concentration) at 90 °C, and 35 min and 25 mL (bleach volume) at 80 °C, respectively, providing pulps with a low Kappa number (<3) and lignin content, and cellulose with a high degree of crystallinity. The H NMR, XRD, FTIR spectroscopy, SEM and thermal analysis demonstrated that it is possible to synthetize cellulose acetate (with 2.62 degrees of substitution) by acetylating bleached pulp for 16 h at 25 °C.

摘要

在合成醋酸纤维素之前,对高粱秸秆的制浆和漂白工艺进行了优化。采用了 2 因素中心复合设计。考虑的变量是制浆的蒸煮时间(1.5 至 2.5 小时)和稀碱浓度(0.75 至 1.25%),以及漂白的漂白时间(30 至 35 分钟)和漂白液体积(20 至 25 毫升)。高粱秸秆由 49.43%的α-纤维素、19.18%的半纤维素和 30.42%的木质素组成。最大程度优化这些工艺的最佳条件分别为 90°C 下 2.5 小时和 1.25%(稀碱浓度),以及 80°C 下 35 分钟和 25 毫升(漂白液体积),得到的纸浆卡伯值较低(<3),木质素含量低,纤维素结晶度高。1H NMR、XRD、FTIR 光谱、SEM 和热分析表明,通过在 25°C 下对漂白后的纸浆乙酰化 16 小时,可以合成取代度为 2.62 的醋酸纤维素。