The purpose of this in vitro study was to determine and compare the shear bond strength and ARI score of one traditional etch-and-rinse adhesive system serving as control, with those of two other all-in-one adhesives but with enamel acid etching preceding their application, and of one new 8th generation all-in-one bonding agent combined with a traditional adhesive used to bond stainless steel buccal tubes to molar teeth.
Four groups of teeth were formulated according to the adhesive system used to bond the tubes on the molars. Shear bond strength was measured using a universal testing machine (Hounsfield, UK). After debonding, each enamel surface was imaged using Inspex HD l080p Vesa camera (Ash Technologies Ltd., Ireland) to determine the ARI score.
The mean SBSs in MPa for the four groups were respectively: A: 9.640 (±3.69), B: 10.261 (±3.03), C: 9.689 (±2.48), D: 8.412 (±3.02). No statistically significant differences were neither found through one-way ANOVA to exist between the group means (P: 0.715), nor for the ARI score frequence through Chi (P: 0.534). Maxcem Elite showed four and G-Premio Bond zero instances of enamel fracture.
1. SBSs of all adhesives and ARI score distributions did not present any significant differences when used to bond stainless steel molar tubes. 2. All adhesives presented with acceptable shear bond strengths for clinical use. 3. Maxcem Elite under the tested conditions presented the greatest and G-Premio the least number of enamel fractures.
本体外研究旨在比较并确定一种传统酸蚀-冲洗型黏接剂(作为对照组)与另外两种全酸蚀黏接剂以及一种新型第 8 代全酸蚀黏接剂与传统黏接剂联合应用于黏接不锈钢颊管至磨牙时的剪切黏结强度(SBS)和黏接剂-牙体界面(ARI)评分。
根据黏接剂系统将牙齿分为 4 组,以黏接颊管至磨牙。使用万能试验机(英国 Hounsfield)测量 SBS。黏接剂去除后,使用 Inspex HD l080p Vesa 相机(爱尔兰 Ash Technologies Ltd.)对每个釉质表面成像,以确定 ARI 评分。
4 组的平均 SBS 值(MPa)分别为:A:9.640(±3.69)、B:10.261(±3.03)、C:9.689(±2.48)、D:8.412(±3.02)。单因素方差分析(one-way ANOVA)未发现组间平均值存在统计学差异(P:0.715),也未发现 ARI 评分频率存在统计学差异(P:0.534)。Maxcem Elite 出现 4 例釉质裂,G-Premio Bond 则为 0 例。