Constantin Marieta, Cosman Bogdan, Bercea Maria, Ailiesei Gabriela-Liliana, Fundueanu Gheorghe
"Petru Poni" Institute of Macromolecular Chemistry, 41-A Gr. Ghica Voda Alley, 700487 Iasi, Romania.
Polymers (Basel). 2021 Sep 7;13(18):3025. doi: 10.3390/polym13183025.
A thermosensitive copolymer composed of amphiphilic triblock copolymer, poloxamer 407, grafted on hydrophilic pullulan with pendant carboxymethyl groups (CMP) was prepared and characterized. The structure of the new copolymer was assessed by Fourier transform infrared (FT-IR) and H nuclear magnetic resonance (H NMR) spectroscopy. The content of the poloxamer in the grafted copolymer was 83.8% (/). The effect of the copolymer concentration on the gelation behavior was analyzed by the vertical method and rheological tests; the gel phase of the copolymer occurred at a lower concentration (11%, /) as compared with poloxamer (18%, /). The starting gelation time under the simulated physiological conditions (phosphate buffer with a pH of 7.4, at 37 °C) was sensitive on the rest temperature before the test, this being 990 s and 280 s after 24 h rest at 4 °C and 20 °C, respectively. The rheological tests evidenced a high elasticity and excellent ability of the copolymer to recover the initial structure after the removal of the applied force or external stimuli. Moreover, the hydrogel has proved a sustained release of amoxicillin (taken as a model drug) over 168 h. Taken together, the results clearly indicate that this copolymer can be used as an injectable hydrogel.
制备并表征了一种热敏共聚物,该共聚物由两亲性三嵌段共聚物泊洛沙姆407接枝到带有羧甲基侧基(CMP)的亲水性支链淀粉上组成。通过傅里叶变换红外光谱(FT-IR)和氢核磁共振光谱(H NMR)对新型共聚物的结构进行了评估。接枝共聚物中泊洛沙姆的含量为83.8%(/)。采用垂直法和流变学测试分析了共聚物浓度对凝胶化行为的影响;与泊洛沙姆(18%,/)相比,该共聚物在较低浓度(11%,/)时出现凝胶相。在模拟生理条件下(pH为7.4的磷酸盐缓冲液,37℃),起始凝胶化时间对测试前的静置温度敏感,在4℃和20℃分别静置24小时后,起始凝胶化时间分别为990秒和280秒。流变学测试表明该共聚物具有高弹性,并且在去除外力或外部刺激后能够很好地恢复初始结构。此外,已证明该水凝胶对阿莫西林(作为模型药物)具有168小时的缓释效果。综上所述,结果清楚地表明这种共聚物可作为可注射水凝胶使用。