A study on the influence of the inclusion of slag or fly ash and five types of superplasticizers on the fresh and hardened properties of alkali-activated cements is presented. Three alkali-activated slag formulations with different fly ash content (0, 15, and 30%) in the presence of five admixtures (vinyl copolymer, melamine, and three polycarboxylates with different chain lengths) were assessed for fluidity control and setting adjustment without loss of mechanical properties. Solid sodium metasilicate was used as an alkaline activator. Their fresh and hardened properties were studied through slump, setting time, isothermal calorimetry, mechanical strengths, and porosity tests. The results showed that the increase of fly ash content delayed the reaction and improved workability but reduced compressive strengths. Concerning the admixtures, these maintained fluidity especially for the one based on polycarboxylate with very long chains. The melamine and polycarboxylate with very long chain admixtures did not have a drastic impact on mechanical properties at early ages; even a gain of flexural and compressive strength was noted.
本文介绍了一项关于矿渣或粉煤灰以及五种类型减水剂的掺入对碱激发水泥新拌及硬化性能影响的研究。评估了在五种外加剂(乙烯基共聚物、三聚氰胺以及三种不同链长的聚羧酸盐)存在的情况下,三种不同粉煤灰含量(0%、15%和30%)的碱激发矿渣配方在不损失力学性能的前提下对流动性控制和凝结调节的效果。使用固体硅酸钠作为碱性激发剂。通过坍落度、凝结时间、等温量热法、力学强度和孔隙率测试来研究它们的新拌及硬化性能。结果表明,粉煤灰含量的增加延迟了反应并改善了工作性,但降低了抗压强度。关于外加剂,它们能保持流动性,尤其是基于非常长链聚羧酸盐的外加剂。三聚氰胺和非常长链聚羧酸盐外加剂在早期对力学性能没有剧烈影响;甚至还观察到抗折和抗压强度有所提高。