Suppr超能文献

预制氧化锆全冠与定制氧化锆全冠在热机械老化后的抗折裂性能:一项体外研究。

Fracture resistance of prefabricated versus custom-made zirconia crowns after thermo-mechanical aging: an in-vitro study.

机构信息

Department of Pediatric Dentistry, Faculty of Dentistry, Cairo University, Cairo, Egypt.

Department of Pediatric Dentistry, Faculty of Dentistry, Fayoum University, Fayoum, Egypt.

出版信息

BMC Oral Health. 2022 Dec 9;22(1):587. doi: 10.1186/s12903-022-02628-x.

Abstract

BACKGROUND

Prefabricated zirconia crowns for a young permanent molar is a child-friendly solution for restoring a permanent molar at a young age. This in-vitro study aimed to compare the fracture resistance of prefabricated versus custom-made permanent molar crowns.

METHODS

16 identical resin dies were fabricated to receive permanent molar zirconia crowns, dies were divided into 2 groups, 1) received perfricated crowns, 2) custom-made crowns. Thermo-dynamic cycling was performed to simulate 6 months in the oral cavity, Fracture resistance of each group was assessed by applying increasing load till fracture. Data were tested for normality using Shapiro-Wilk and Levene's tests. Data were analyzed using independent t test.

RESULTS

No statistically significant difference was found between fracture resistance of prefabricated and custom-made crowns (1793.54 ± 423.82) and (1987.38 ± 414.88) respectively. 3 crowns of the custom-made group fractured with the underlying die, versus zero dies fractured in the prefabricated group.

CONCLUSIONS

Prefabricated permanent molars zirconia crowns can perform as well as custom-made crowns for an adult in terms of fracture resistance, it is suitable for children and can withstand the occlusal forces of an adult.

摘要

背景

预制氧化锆冠修复年轻恒牙是一种对儿童友好的解决方案,可在早期恢复恒牙。本体外研究旨在比较预制和定制永久磨牙冠的抗折能力。

方法

制作 16 个相同的树脂模型以接收永久磨牙氧化锆冠,将模型分为 2 组,1)接收预制冠,2)定制冠。进行热动力学循环以模拟口腔中的 6 个月,通过施加递增的负载直到断裂来评估每组的抗断裂能力。使用 Shapiro-Wilk 和 Levene 检验测试数据的正态性。使用独立 t 检验分析数据。

结果

预制和定制冠的抗折能力无统计学差异(分别为 1793.54 ± 423.82)和(1987.38 ± 414.88)。定制组的 3 个冠与基础模具一起断裂,而预制组没有模具断裂。

结论

预制的永久磨牙氧化锆冠在抗折能力方面可以与成人定制冠一样,适合儿童使用,并能承受成人的咬合力量。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/9eeb/9733029/f322fbc08bbe/12903_2022_2628_Fig1_HTML.jpg

相似文献

2
Custom-made versus prefabricated zirconia crowns for primary molars: A 12-month follow-up.
J Indian Soc Pedod Prev Dent. 2024 Apr 1;42(2):156-164. doi: 10.4103/jisppd.jisppd_39_24. Epub 2024 Jun 28.
3
Fracture strength of preformed zirconia crown and new custom-made zirconia crown for the restoration of deciduous molars: in vitro study.
Eur Arch Paediatr Dent. 2022 Apr;23(2):333-339. doi: 10.1007/s40368-022-00691-0. Epub 2022 Jan 25.
5
Fracture load and chewing simulation of zirconia and stainless-steel crowns for primary molars.
Eur J Oral Sci. 2019 Aug;127(4):369-375. doi: 10.1111/eos.12645. Epub 2019 Jul 10.
7
Effect of supporting dies' mechanical properties on fracture behavior of monolithic zirconia molar crowns.
Dent Mater J. 2022 Apr 1;41(2):249-255. doi: 10.4012/dmj.2021-090. Epub 2021 Dec 4.
8
Fracture resistance of monolithic zirconia molar crowns with reduced thickness.
Acta Odontol Scand. 2015;73(8):602-8. doi: 10.3109/00016357.2015.1007479. Epub 2015 Jan 30.
9
Mechanical stability of fully personalized, abutment-free zirconia implant crowns on a novel implant-crown interface.
J Dent. 2022 Jun;121:104121. doi: 10.1016/j.jdent.2022.104121. Epub 2022 Apr 5.
10
Fracture Resistance Behaviors of Titanium-Zirconium and Zirconia Implants.
J Prosthodont. 2022 Jun;31(5):441-446. doi: 10.1111/jopr.13440. Epub 2021 Oct 30.

引用本文的文献

1
Strategies for Restoration of Compromised First Permanent Molars in Children: Challenges and Optimal Timing.
Oral Health Prev Dent. 2025 Aug 8;23:435-446. doi: 10.3290/j.ohpd.c_2175.
3
The influence of cavity design on the mechanical behavior of endo-crown restorations: an ex-vivo study.
BMC Oral Health. 2025 Jul 19;25(1):1214. doi: 10.1186/s12903-025-06586-y.
9
Qualitative surface roughness of lithium disilicate endo-crown for pulpotomized primary molars.
Sci Rep. 2024 Aug 11;14(1):18640. doi: 10.1038/s41598-024-68689-w.

本文引用的文献

1
Zirconia Crowns for Primary Teeth: A Systematic Review and Meta-Analyses.
Int J Environ Res Public Health. 2022 Feb 28;19(5):2838. doi: 10.3390/ijerph19052838.
2
Fatigue Resistance of 3-Unit CAD-CAM Ceramic Fixed Partial Dentures: An FEA Study.
J Prosthodont. 2022 Dec;31(9):806-814. doi: 10.1111/jopr.13487. Epub 2022 Feb 22.
3
Comparison of Fracture Load of the Four Translucent Zirconia Crowns.
Molecules. 2021 Sep 1;26(17):5308. doi: 10.3390/molecules26175308.
4
Zirconia crowns for children: A systematic review.
Int J Paediatr Dent. 2022 Jan;32(1):66-81. doi: 10.1111/ipd.12793. Epub 2021 Apr 25.
5
Prefabricated Zirconia Crowns - A Solution to Treat Hypomineralized Permanent Molars: Report of a Case.
J Clin Pediatr Dent. 2021 Jan 1;45(1):8-11. doi: 10.17796/1053-4625-45.1.2.
7
Retrieval of Prefabricated Zirconia Crowns with Er,Cr:YSGG Laser from Primary and Permanent Molars.
Materials (Basel). 2020 Dec 7;13(23):5569. doi: 10.3390/ma13235569.
8
Post-fatigue fracture resistance of premolar teeth restored with endocrowns: An in vitro investigation.
J Dent. 2020 Sep;100:103426. doi: 10.1016/j.jdent.2020.103426. Epub 2020 Jul 3.
10
Molar hypomineralization: What is the US experience?
J Am Dent Assoc. 2018 May;149(5):329-330. doi: 10.1016/j.adaj.2018.03.013.

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验