Slovenian National Building and Civil Engineering Institute, Dimičeva Ulica 12, Ljubljana, Slovenia.
Sci Rep. 2023 Feb 24;13(1):3245. doi: 10.1038/s41598-023-28971-9.
CoCrMo and Ti6Al4V are widely used in medical, dental and 3D printing technology, allowing the accurate fabrication of geometrically complicated structures. In order to reduce the costs of printed objects, the reuse of powder is common daily practice. When using 3D printing technology, the direct impact of elevated temperatures and the influence of the laser beam may change the properties of the powder when it is reused, thus affecting the final properties of the printed object. The main aim of the present study was to investigate the impact of reused powder on the mechanical, microstructural and electrochemical properties of 3D printed objects. 3D printed objects fabricated from virgin and reused powder of both alloys were analyzed by metallographic observation, computed tomography, XRD and electrochemical methods. The main finding of the study was that the use of reused powder (recycled 3 times) does not detrimentally affect the mechanical and corrosion integrity of 3D printed CoCr and Ti6Al4V alloys, especially for the purpose of applications in dentistry.
CoCrMo 和 Ti6Al4V 广泛应用于医疗、牙科和 3D 打印技术领域,可精确制造出几何形状复杂的结构。为了降低打印物体的成本,粉末的再利用是常见的日常做法。在使用 3D 打印技术时,升高的温度的直接影响和激光束的影响可能会改变再利用粉末的特性,从而影响打印物体的最终性能。本研究的主要目的是研究再利用粉末对 3D 打印物体的机械、微观结构和电化学性能的影响。通过金相观察、计算机断层扫描、XRD 和电化学方法对由两种合金的原始粉末和再利用粉末制造的 3D 打印物体进行了分析。研究的主要发现是,再利用粉末(回收 3 次)的使用不会对 3D 打印 CoCr 和 Ti6Al4V 合金的机械和腐蚀完整性产生不利影响,尤其是在牙科应用方面。