Alaqeely Razan, Bukhamseen Rabab, Alshehri Reema, Alsayed Hussain, Matinlinna Jukka, Alhotan Abdulaziz
Department of Periodontics and Community Dentistry, College of Dentistry, King Saud University, Riyadh, 12372, Saudi Arabia.
Postgraduate, Johns Hopkins University, Baltimore, MD 21218, United States.
Heliyon. 2024 Jul 26;10(15):e35241. doi: 10.1016/j.heliyon.2024.e35241. eCollection 2024 Aug 15.
This pilot study evaluated the immediate effect of different herbal solutions in oral use on the tensile strength of the sutures used in oral surgical procedures. Three frequently used suture materials, polyglactin 910 (PGA), poliglecaprone (PGCL), and polypropylene (PP), were chosen in a 4-0-gauge size. The sutures' tensile stress was evaluated before being immersed (baseline) and after immersion at 24 h, 1 week, and 2 weeks in four different media: artificial saliva, chlorhexidine, Commiphora myrrh, and frankincense. The tensile strength was assessed by applying a 50 N load at a standardized speed of 2 mm/min. The data were analyzed using one-way and three-way analysis of variance (ANOVA) and the Tukey test with a significance level of p ≤ 0.05 significance level. The mean values of the maximum load showed a significant statistical difference across the three types of sutures (PGA, PGCL, and PP). The mean tensile strength of the PP suture was statistically lower than that of the other sutures. There was a statistically significant difference in the mean tensile strength of the PGA suture when stored in chlorohexidine media and the PGCL suture for frankincense media. The tensile strength for all sutures was the lowest value when immersed in Commiphora myrrh media. Home-prepared herbal solutions can affect the tensile strength and maximum load of suture materials. Careful and controlled use of herbal solutions after any dental surgical procedures is advisable.
这项初步研究评估了不同口腔用草药溶液对口腔外科手术中使用的缝线拉伸强度的即时影响。选择了三种常用的缝线材料,4-0规格的聚乙醇酸910(PGA)、聚甘醇碳酸(PGCL)和聚丙烯(PP)。在四种不同介质(人工唾液、氯己定、没药和乳香)中,在浸入前(基线)以及浸入24小时、1周和2周后评估缝线的拉伸应力。通过以2毫米/分钟的标准速度施加50牛的负荷来评估拉伸强度。使用单向和三向方差分析(ANOVA)以及显著性水平为p≤0.05的Tukey检验对数据进行分析。三种缝线类型(PGA、PGCL和PP)的最大负荷平均值显示出显著的统计学差异。PP缝线的平均拉伸强度在统计学上低于其他缝线。当PGA缝线储存在氯己定介质中以及PGCL缝线储存在乳香介质中时,其平均拉伸强度存在统计学显著差异。所有缝线浸入没药介质时的拉伸强度最低。自制草药溶液会影响缝线材料的拉伸强度和最大负荷。在任何牙科手术后谨慎且有控制地使用草药溶液是明智的。